Melola Discovery

← Melola Discovery

Akses terbuka Jurnal SINTA 1

Monitoring Low-Cycle Fatigue Material-Degradation by Ultrasonic Methods

Atom Indonesia · Vol. 36 No. 2 (2011) · hlm. 63–68

DOI
10.17146/aij.2010.26
ISSN
2356-5322, 0126-1568
Terbit
2011-09-08
Penerbit
National Research and Innovation Agency
Bahasa
eng
Lisensi
creativecommons.org/licenses/by-nc-sa/4.0

Abstrak

Any system consisting of structural material often undergoes fatigue, which is caused by dynamic load cycle. As a structural system, nuclear power plant is very likely to have low-cycle fatigue at many of its components. Taking into account the importance of monitoring low-cycle fatigue on structural components to prevent them from getting failure, the authors have conducted a work to monitor material degradation caused by low-cycle fatigue by using ultrasonic method. An alloy of Cu-40Zn was used as a test specimen. Ultrasonic water immersion procedure was employed in this ultrasonic test. The probe used is a focusing type and has frequency as high as 15 MHz. The specimen area tested is in the middle part divided into 14 points × 23 points. The results, which were frequency spectrums, were analyzed using two parameters: frequency spectrum peak intensity and attenuation function gradient. The analysis indicates that peak intensity increases at the beginning of load cycle and then decreases. Meanwhile, gradient of attenuation function is lower at the beginning of fatigue process, and then consistently gets higher. It concludes that low-fatigue material degradation can be monitored by using ultrasonic method.Received: 20 November 2009; Revised: 31 August 2010; Accepted: 31 August 2010

Kata kunci

Jaringan kolaborasi para penulis

3 penulis · 3 tautan kepenulisan bersama · 2 lintas organisasi

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • National Nuclear Energy Agency of Indonesia
  • Saitama University
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OAI-PMH (metadata jurnal) https://atomindonesia.brin.go.id/index.php/aij/oai, pertama di-harvest 8 Nov 2026, terakhir terlihat 22 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/  http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
	<dc:title xml:lang="en-US">Monitoring Low-Cycle Fatigue Material-Degradation by Ultrasonic Methods</dc:title>
	<dc:creator>Himawan, R.</dc:creator>
	<dc:creator>Katoh, H.</dc:creator>
	<dc:creator>Cahyono, A.</dc:creator>
	<dc:subject xml:lang="en-US">Low-cycle fatigue; Non-destructive test;  Ultrasonic method</dc:subject>
	<dc:description xml:lang="en-US">Any system consisting of structural material often undergoes fatigue, which is caused by dynamic load cycle. As a structural system, nuclear power plant is very likely to have low-cycle fatigue at many of its components. Taking into account the importance of monitoring low-cycle fatigue on structural components to prevent them from getting failure, the authors have conducted a work to monitor material degradation caused by low-cycle fatigue by using ultrasonic method. An alloy of Cu-40Zn was used as a test specimen. Ultrasonic water immersion procedure was employed in this ultrasonic test. The probe used is a focusing type and has frequency as high as 15 MHz. The specimen area tested is in the middle part divided into 14 points × 23 points. The results, which were frequency spectrums, were analyzed using two parameters: frequency spectrum peak intensity and attenuation function gradient. The analysis indicates that peak intensity increases at the beginning of load cycle and then decreases. Meanwhile, gradient of attenuation function is lower at the beginning of fatigue process, and then consistently gets higher. It concludes that low-fatigue material degradation can be monitored by using ultrasonic method.Received: 20 November 2009; Revised: 31 August 2010; Accepted: 31 August 2010</dc:description>
	<dc:publisher xml:lang="en-US">National Research and Innovation Agency</dc:publisher>
	<dc:contributor xml:lang="en-US">National Nuclear Energy Agency of Indonesia</dc:contributor>
	<dc:date>2011-09-08</dc:date>
	<dc:type>info:eu-repo/semantics/article</dc:type>
	<dc:type>info:eu-repo/semantics/publishedVersion</dc:type>
	<dc:type xml:lang="en-US"></dc:type>
	<dc:format>application/pdf</dc:format>
	<dc:identifier>https://atomindonesia.brin.go.id/index.php/aij/article/view/26</dc:identifier>
	<dc:identifier>10.17146/aij.2010.26</dc:identifier>
	<dc:source xml:lang="en-US">Atom Indonesia; Vol 36, No 2 (2010): August 2010; 63-68</dc:source>
	<dc:source>2356-5322</dc:source>
	<dc:source>0126-1568</dc:source>
	<dc:source>10.17146/aij.2010.%x</dc:source>
	<dc:language>eng</dc:language>
	<dc:relation>https://atomindonesia.brin.go.id/index.php/aij/article/view/26/18</dc:relation>
	<dc:rights xml:lang="en-US">Copyright (c) 2016 Atom Indonesia</dc:rights>
	<dc:rights xml:lang="en-US">http://creativecommons.org/licenses/by-nc-sa/4.0</dc:rights>
</oai_dc:dc>