Photocatalytic Degradation of Remazol Brilliant Blue R and Remazol Yellow FG using TiO2 doped Cd, Co, Mn

Bulletin of Chemical Reaction Engineering & Catalysis · Vol. ume (2021) · hlm. 804–815

DOI
10.9767/bcrec.16.4.11423.804-815
ISSN
1978-2993
Terbit
2021-12-20
Penerbit
Masyarakat Katalis Indonesia - Indonesian Catalyst Society (MKICS)
Bahasa
eng
Lisensi
creativecommons.org/licenses/by-sa/4.0

Abstrak

TiO2 and TiO2 doped Cd, Co, Mn (TiO2-M) were synthesized with a sol-gel method, and the photocatalytic activity of Remazol Brilliant Blue R and Remazol Yellow FG has been conducted. TiO2-M (Cd, Co, Mn) was synthesized with the mol Ti:M ratio of 3:1, and the materials were calcined at 300, 400, and 500 °C. The materials were characterized by X-ray Diffraction (XRD), Scanning Electron Microscopy-Energy Dispersive X-ray (SEM-EDX), and UV-Vis Reflectance. The XRD result shows that at the temperature of 300 °C TiO2 and TiO2-M formed tend to be amorphous. At 400 °C the anatase phase is formed, while at 500 °C the rutile phase begins to form. And overall, the crystallinity of TiO2 is higher than metal-doped TiO2. The UV-Vis Reflectance result showed that the bandgap energy of all doping materials (TiO2-M) decreased. The larger the metal ion radius of dopant, the larger the crystal size obtained and then the higher the bandgap obtained. The results of SEM-EDX showed that the morphology of TiO2 was spherical and regular, whereas the morphology of TiO2-M had a smoother surface due to the influence of metal doping. Photocatalytic activity of TiO2-M on Remazol Brilliant Blue R and Remazol Yellow FG was greater than TiO2. The optimum pH of the solution was obtained at pH 5 and the optimum catalyst phase was obtained at the anatase phase. The percentages degradation for 30 min of Remazol Brilliant Blue R were 67.34% (TiO2), 92.12% (TiO2-Co), 85.47% (TiO2-Mn), and 83.91% (TiO2-Cd), while for Remazol Yellow FG they were 58.84% (TiO2), 74.61% (TiO2-Co), 67.93% (TiO2-Mn) and 64.19% (TiO2-Cd), respectively. Copyright © 2021 by Authors, Published by BCREC Group. This is an open access article under the CC BY-SA License (https://creativecommons.org/licenses/by-sa/4.0).

Kata kunci

Jaringan kolaborasi para penulis

29 penulis · 87 tautan kepenulisan bersama · 5 lintas organisasi

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • Sebelas Maret University
  • Indonesia University of Education
  • Afiliasi tidak diketahui
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama
Ozi Adi SaputraSebelas Maret University3
Fitri N. AiniSebelas Maret University2
Vaishnavita NawakusumaSebelas Maret University2
Erick Ryan YuliantoSebelas Maret University2
Rochmad E. CahyonoSebelas Maret University1
Fitria RahmawatiSebelas Maret University1
Dian IriantiSebelas Maret University1
Betty NurhayatiSebelas Maret University1
KurniaSebelas Maret University1
Septi PujiasihSebelas Maret University1
Vanani Nur RizkiSebelas Maret University1
Edi Priyo PramonoSebelas Maret University1
Tri MartiniIndonesia University of Education1
Sri HastutiSebelas Maret University1
E N FajarianiSebelas Maret University1
Intan K. CandraningrumSebelas Maret University1
Witri Wahyu LestariSebelas Maret University1
Widyan Muhammad NaufalSebelas Maret University1
Teguh Endah SaraswatiSebelas Maret University1
Sri HastutiSebelas Maret University1
Hasna Haifa IrfaniAfiliasi tidak diketahui1
Rifania Aura NuzulaAfiliasi tidak diketahui1
Abu MasykurAfiliasi tidak diketahui1
Atmanto Heru WibowoAfiliasi tidak diketahui1
Dina FitrianaAfiliasi tidak diketahui1

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OAI-PMH (metadata jurnal) https://journal.bcrec.id/index.php/bcrec/oai, pertama di-harvest 8 Nov 2026, terakhir terlihat 8 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/  http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
	<dc:title xml:lang="en-US">Photocatalytic Degradation of Remazol Brilliant Blue R and Remazol Yellow FG using TiO2 doped Cd, Co, Mn</dc:title>
	<dc:creator>Purnawan, Candra</dc:creator>
	<dc:creator>Wahyuningsih, Sayekti</dc:creator>
	<dc:creator>Aniza, Oktaviani Nur</dc:creator>
	<dc:creator>Sari, Octaria Priwidya</dc:creator>
	<dc:subject xml:lang="en-US">Degradation; Remazol Brilliant Blue R; Remazol Yellow FG,;TiO2; TiO2-M (Cd, Co, Mn)</dc:subject>
	<dc:description xml:lang="en-US">TiO2 and TiO2 doped Cd, Co, Mn (TiO2-M) were synthesized with a sol-gel method, and the photocatalytic activity of Remazol Brilliant Blue R and Remazol Yellow FG has been conducted. TiO2-M (Cd, Co, Mn) was synthesized with the mol Ti:M ratio of 3:1, and the materials were calcined at 300, 400, and 500 °C. The materials were characterized by X-ray Diffraction (XRD), Scanning Electron Microscopy-Energy Dispersive X-ray (SEM-EDX), and UV-Vis Reflectance. The XRD result shows that at the temperature of 300 °C TiO2 and TiO2-M formed tend to be amorphous. At 400 °C the anatase phase is formed, while at 500 °C the rutile phase begins to form. And overall, the crystallinity of TiO2 is higher than metal-doped TiO2. The UV-Vis Reflectance result showed that the bandgap energy of all doping materials (TiO2-M) decreased. The larger the metal ion radius of dopant, the larger the crystal size obtained  and then the higher the bandgap obtained. The results of SEM-EDX showed that the morphology of TiO2 was spherical and regular, whereas the morphology of TiO2-M had a smoother surface due to the influence of metal doping. Photocatalytic activity of TiO2-M on Remazol Brilliant Blue R and Remazol Yellow FG was greater than TiO2. The optimum pH of the solution was obtained at pH 5 and the optimum catalyst phase was obtained at the anatase phase. The percentages degradation for 30 min of Remazol Brilliant Blue R were 67.34% (TiO2), 92.12% (TiO2-Co), 85.47% (TiO2-Mn), and 83.91% (TiO2-Cd), while for Remazol Yellow FG they were 58.84% (TiO2), 74.61% (TiO2-Co), 67.93% (TiO2-Mn) and 64.19% (TiO2-Cd), respectively. Copyright © 2021 by Authors, Published by BCREC Group. This is an open access article under the CC BY-SA License (https://creativecommons.org/licenses/by-sa/4.0). </dc:description>
	<dc:publisher xml:lang="en-US">Masyarakat Katalis Indonesia - Indonesian Catalyst Society (MKICS)</dc:publisher>
	<dc:date>2021-12-20</dc:date>
	<dc:type>info:eu-repo/semantics/article</dc:type>
	<dc:type>info:eu-repo/semantics/publishedVersion</dc:type>
	<dc:type xml:lang="en-US"></dc:type>
	<dc:format>application/pdf</dc:format>
	<dc:identifier>https://journal.bcrec.id/index.php/bcrec/article/view/11423</dc:identifier>
	<dc:identifier>10.9767/bcrec.16.4.11423.804-815</dc:identifier>
	<dc:source xml:lang="en-US">Bulletin of Chemical Reaction Engineering &amp; Catalysis; 2021: BCREC Volume 16 Issue 4 Year 2021 (December 2021); 804-815</dc:source>
	<dc:source>1978-2993</dc:source>
	<dc:language>eng</dc:language>
	<dc:relation>https://journal.bcrec.id/index.php/bcrec/article/view/11423/6246</dc:relation>
	<dc:rights xml:lang="en-US">Copyright (c) 2021 by Authors, Published by BCREC Group</dc:rights>
	<dc:rights xml:lang="en-US">https://creativecommons.org/licenses/by-sa/4.0</dc:rights>
</oai_dc:dc>