Cytotoxicity difference of 316L stainless steel and titanium reconstruction plate

Dental Journal (Majalah Kedokteran Gigi) · Vol. 44 No. 1 (2011) · hlm. 7–11

DOI
10.20473/j.djmkg.v44.i1.p7-11
ISSN
2442-9740, 1978-3728
Terbit
2011-03-01
Penerbit
Faculty of Dental Medicine, Universitas Airlangga https://fkg.unair.ac.id/en
Bahasa
eng

Abstrak

Background: Pure titanium is the most biocompatible material today and used as a gold standard for metallic implants. However, stainless steel is still being used as implants because of its strength, ductility, lower price, corrosion resistant and biocompatibility. Purpose: This study was done to revealed the cytotoxicity difference between reconstruction plate made of 316L stainless steel and of commercially pure (CP) titanium in baby hamster kidney-21 (BHK-21) fibroblast culture through MTT assay. Methods: Eight samples were prepared from reconstruction plates made of stainless steel type 316L grade 2 (Coen's reconstruction plate®) that had been cut into cylindrical form of 2 mm in diameter and 3 mm long. The other one were made of CP titanium (STEMA Gmbh®)) of 2 mm in diameter and 2,2 mm long; and had been cleaned with silica paper and ultrasonic cleaner, and sterilized in autoclave at 121° C for 20 minutes.9 Both samples were bathed into microplate well containing 50 μl of fibroblast cells with 2 x 105 density in Rosewell Park Memorial Institute-1640 (RPMI-1640) media, spinned at 30 rpm for 5 minutes. Microplate well was incubated for 24 and 48 hours in 37° C. After 24 hours, each well that will be read at 24 hour were added with 50 μl solution containing 5mg/ml MTT reagent in phosphate buffer saline (PBS) solutions, then reincubated for 4 hours in CO2 10% and 37° C. Colorometric assay with MTT was used to evaluate viability of the cells population after 24 hours. Then, each well were added with 50 μl dimethyl sulfoxide (DMSO) and reincubated for 5 minutes in 37° C. the wells were read using Elisa reader in 620 nm wave length. Same steps were done for the wells that will be read in 48 hours. Each data were tabulated and analyzed using independent T-test with significance of 5%. Results: This study showed that the percentage of living fibroblast after exposure to 316L stainless steel reconstruction plate was 61.58% after 24 hours and 62.33% after 48 hours. And after exposure to titanium reconstruction plate, the percentage of living fibroblast was 98.69% after 24 hours and 82.24% after 48 hours. Based on cytotoxicity parameter (CD50%), both reconstruction plate made of 316L stainless steel or titanium showed as a non-toxic materials to fibroblast. Conclusion: Both reconstruction plate made of stainless steel and CP titanium were non-toxic to fibroblast, although the stainless steel plate showed lower cytotoxicity level compared to titanium. Therefore a reconstruction plate made from stainless steel type 316L can be used as a safe material for mandibular reconstruction. Latar belakang: Titanium murni adalah bahan yang paling biokompatibel saat ini dan digunakan sebagai standar emas implan logam. Saat ini stainless steel masih digunakan karena kekuatan, ductility, harganya yang murah, tahan terhadap korosi dan cukup biokompatibel. Tujuan: Penelitian ini dilakukan untuk mengetahui perbedaan sitotoksisitas antara plat rekonstruksi yang terbuat dari titanium murni komersial dan plat rekonstruksi yang terbuat dari stainless steel pada kultur sel fibroblas baby hamster kidney-21 (BHK-21) menggunakan MTT assay. Metode: Delapan sampel yang masing-masing tipe 316L terbuat dari stainless steel 316L grade 2 (Coen's reconstruction plate®) yang dipotong berbentuk silinder diameter 2 mm dan panjang 3 mm, serta yang terbuat dari titanium murni komersial (STEMA Gmbh®) diameter 2 mm dan panjang 2,2 mm; dan dibersihkan dengan kertas silika dan pembersih ultrasonik serta disterilkan dengan autoclave pada suhu 121° C selama 20 menit. Kedua sampel dimasukkan ke dalam sumur mikroplat yang mengandung 50 μl sel fibroblas dengan kepadatan 2 í— 105 dalam media Rosewell Park Memorial Institute-1640 (RPMI-1640), diputar dengan kecepatan 30 rpm selama 5 menit. Sumur mikroplat diinkubasi selama 24 dan 48 jam pada suhu 37° C. Setelah 24 "> jam, pada tiap sumur yang akan dibaca pada jam ke 24 ditambahkan 50 μl cairan yang mengandung 5mg/ml MTT dalam phosphat buffer saline (PBS), kemudian diinkubasi kembali selama 4 jam dalam CO2 10% pada suhu 37° C. Assay kolorimetri dengan MTT digunakan untuk mengetahui viabilitas populasi sel setelah 24 jam. Setiap sumur ditambahkan pelarut dimetil sulfoksida (DMSO) dan diinkubasi kembali selama 5 menit pada suhu 37° C. sumur-sumur tersebut kemudian dibaca dengan Elisa reader dengan panjang gelombang 620 nm. Langkah yang sama dilakukan pada sumur-sumur yang akan dibaca pada jam ke 48. Data kemudian ditabulasi dan dianalisis dengan menggunakan independent T-test dengan signifikansi 5%. Hasil: Penelitian ini menunjukkan presentase fibroblas hidup setelah terpapar plat rekonstruksi yang terbuat dari stainless steel adalah 61,58% setelah 24 jam dan 62,33% setelah 48 jam. Dan setelah paparan dengan plat rekonstruksi yang terbuat dari titanium murni adalah 98,69% setelah 24 jam dan 82,24% setelah 48 jam. Berdasarkan pada parameter sitotoksisitas (CD50%) kedua plat rekonstruksi baik yang terbuat dari titanium murni maupun yang terbuat dari stainless steel tipe 316L merupakan bahan yang tidak bersifat toksik terhadap fibroblas. Kesimpulan: Kedua plat rekonstruksi baik yang terbuat dari stainless steel maupun CP titanium tidak bersifat toksik terhadap fibroblas, walaupun plat stainless steel menunjukkan level sitotoksisitas yang lebih rendah daripada titanium murni. Dengan demikian plat rekonstruksi yang terbuat dari stainless steel 316 L aman digunakan sebagai bahan untuk rekonstruksi mandibula.

Kata kunci

Jaringan kolaborasi para penulis

40 penulis · 103 tautan kepenulisan bersama · 27 lintas organisasi

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • Universitas Airlangga
  • Universitas Hang Tuah
  • State University of Semarang
  • Lambung Mangkurat University
  • Universitas Malahayati
  • Melmaruvathur Adhiparasakthi Institute of Medical Sciences and Research
  • Universitas Gadjah Mada
  • Organisasi lain
  • Afiliasi tidak diketahui
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama
David Buntoro KamadjajaUniversitas Airlangga4
Istiati IstiatiUniversitas Airlangga3
Christian KhoswantoUniversitas Airlangga3
Ira ArundinaUniversitas Airlangga3
Coen PramonoUniversitas Airlangga2
Nita NaomiUniversitas Airlangga2
Sisca Meida WatiUniversitas Airlangga1
Wisnu Setyari JUniversitas Airlangga1
Fitria RahmitasariUniversitas Hang Tuah1
Jenny SunarianiUniversitas Airlangga1
Agniz Nur AuliaUniversitas Airlangga1
Yuliati YuliatiState University of Semarang1
Dian Widya DamaiyantiUniversitas Hang Tuah1
Dania MaharaniUniversitas Airlangga1
Gunawan OentaryoLambung Mangkurat University1
R. Aries MuharramUniversitas Airlangga1
Zhafira Nur ShabrinaUniversitas Airlangga1
Anggy PrayudhaUniversitas Airlangga1
Roberto M. SimandjuntakUniversitas Airlangga1
Darin Hulwani RinaldiUniversitas Airlangga1
Ganendra AnugrahaUniversitas Airlangga1
Olivia Jennifer GunardiUniversitas Airlangga1
Riska DianaUniversitas Airlangga1
Agung SosiawanUniversitas Airlangga1
Mala KurniatiUniversitas Malahayati1
Dian Agustin WahjuningrumUniversitas Airlangga1
Indra MulyawanUniversitas Airlangga1
Retno Pudji RahayuUniversitas Airlangga1
Muhammad Subhan AmirUniversitas Airlangga1
Septian PradanaUniversitas Airlangga1
James Antony BhagatMelmaruvathur Adhiparasakthi Institute of Medical Sciences and Research1
Rafael GerrardUniversitas Airlangga1
Yoakim Leok TaboyAfiliasi tidak diketahui1
Agatha Sherly Ivana DewiUniversitas Gadjah Mada1
Aurelia Graceilla Putri NindyatamaPelita Harapan University1
Moses Amadeus SoetantoAfiliasi tidak diketahui1

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OAI-PMH (metadata jurnal) https://e-journal.unair.ac.id/MKG/oai, pertama di-harvest 8 Nov 2026, terakhir terlihat 8 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/  http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
	<dc:title xml:lang="en-US">Cytotoxicity difference of 316L stainless steel and titanium reconstruction plate</dc:title>
	<dc:creator>Sumarta, Ni Putu Mira</dc:creator>
	<dc:creator>Danudiningrat, Coen Pramono</dc:creator>
	<dc:creator>Rachmat, Ester Arijani</dc:creator>
	<dc:creator>Soesilawati, Pratiwi</dc:creator>
	<dc:subject xml:lang="en-US">316L Stainless steel plate</dc:subject>
	<dc:subject xml:lang="en-US">titanium plate</dc:subject>
	<dc:subject xml:lang="en-US">cyototoxicity</dc:subject>
	<dc:subject xml:lang="en-US">MTT assay</dc:subject>
	<dc:subject xml:lang="en-US">Plat stainless steel</dc:subject>
	<dc:subject xml:lang="en-US">plat titanium</dc:subject>
	<dc:subject xml:lang="en-US">sitotoksisitas</dc:subject>
	<dc:description xml:lang="en-US">Background: Pure titanium is the most biocompatible material today and used as a gold standard for metallic implants. However, stainless steel is still being used as implants because of its strength, ductility, lower price, corrosion resistant and biocompatibility. Purpose: This study was done to revealed the cytotoxicity difference between reconstruction plate made of 316L stainless steel and of commercially pure (CP) titanium in baby hamster kidney-21 (BHK-21) fibroblast culture through MTT assay. Methods: Eight samples were prepared from reconstruction plates made of stainless steel type 316L grade 2 (Coen's reconstruction plate®) that had been cut into cylindrical form of 2 mm in diameter and 3 mm long. The other one were made of CP titanium (STEMA Gmbh®)) of 2 mm in diameter and 2,2 mm long; and had been cleaned with silica paper and ultrasonic cleaner, and sterilized in autoclave at 121° C for 20 minutes.9 Both samples were bathed into microplate well containing 50 μl of fibroblast cells with 2 x 105 density in Rosewell Park Memorial Institute-1640 (RPMI-1640) media, spinned at 30 rpm for 5 minutes. Microplate well was incubated for 24 and 48 hours in 37° C. After 24 hours, each well that will be read at 24 hour were added with 50 μl solution containing 5mg/ml MTT reagent in phosphate buffer saline (PBS) solutions, then reincubated for 4 hours in CO2 10% and 37° C. Colorometric assay with MTT was used to evaluate viability of the cells population after 24 hours. Then, each well were added with 50 μl dimethyl sulfoxide (DMSO) and reincubated for 5 minutes in 37° C. the wells were read using Elisa reader in 620 nm wave length. Same steps were done for the wells that will be read in 48 hours. Each data were tabulated and analyzed using independent T-test with significance of 5%. Results: This study showed that the percentage of living fibroblast after exposure to 316L stainless steel reconstruction plate was 61.58% after 24 hours and 62.33% after 48 hours. And after exposure to titanium reconstruction plate, the percentage of living fibroblast was 98.69% after 24 hours and 82.24% after 48 hours. Based on cytotoxicity parameter (CD50%), both reconstruction plate made of 316L stainless steel or titanium showed as a non-toxic materials to fibroblast. Conclusion: Both reconstruction plate made of stainless steel and CP titanium were non-toxic to fibroblast, although the stainless steel plate showed lower cytotoxicity level compared to titanium. Therefore a reconstruction plate made from stainless steel type 316L can be used as a safe material for mandibular reconstruction. Latar belakang: Titanium murni adalah bahan yang paling biokompatibel saat ini dan digunakan sebagai standar emas implan logam. Saat ini stainless steel masih digunakan karena kekuatan, ductility, harganya yang murah, tahan terhadap korosi dan cukup biokompatibel. Tujuan: Penelitian ini dilakukan untuk mengetahui perbedaan sitotoksisitas antara plat rekonstruksi yang terbuat dari titanium murni komersial dan plat rekonstruksi yang terbuat dari stainless steel pada kultur sel fibroblas baby hamster kidney-21 (BHK-21) menggunakan MTT assay. Metode: Delapan sampel yang masing-masing tipe 316L terbuat dari stainless steel 316L grade 2 (Coen's reconstruction plate®) yang dipotong berbentuk silinder diameter 2 mm dan panjang 3 mm, serta yang terbuat dari titanium murni komersial (STEMA Gmbh®) diameter 2 mm dan panjang 2,2 mm; dan dibersihkan dengan kertas silika dan pembersih ultrasonik serta disterilkan dengan autoclave pada suhu 121° C selama 20 menit. Kedua sampel dimasukkan ke dalam sumur mikroplat yang mengandung 50 μl sel fibroblas dengan kepadatan 2 í— 105 dalam media Rosewell Park Memorial Institute-1640 (RPMI-1640), diputar dengan kecepatan 30 rpm selama 5 menit. Sumur mikroplat diinkubasi selama 24 dan 48 jam pada suhu 37° C. Setelah 24 "&amp;gt; jam, pada tiap sumur yang akan dibaca pada jam ke 24 ditambahkan 50 μl cairan yang mengandung 5mg/ml MTT dalam phosphat buffer saline (PBS), kemudian diinkubasi kembali selama 4 jam dalam CO2 10% pada suhu 37° C. Assay kolorimetri dengan MTT digunakan untuk mengetahui viabilitas populasi sel setelah 24 jam. Setiap sumur ditambahkan pelarut dimetil sulfoksida (DMSO) dan diinkubasi kembali selama 5 menit pada suhu 37° C. sumur-sumur tersebut kemudian dibaca dengan Elisa reader dengan panjang gelombang 620 nm. Langkah yang sama dilakukan pada sumur-sumur yang akan dibaca pada jam ke 48. Data kemudian ditabulasi dan dianalisis dengan menggunakan independent T-test dengan signifikansi 5%. Hasil: Penelitian ini menunjukkan presentase fibroblas hidup setelah terpapar plat rekonstruksi yang terbuat dari stainless steel adalah 61,58% setelah 24 jam dan 62,33% setelah 48 jam. Dan setelah paparan dengan plat rekonstruksi yang terbuat dari titanium murni adalah 98,69% setelah 24 jam dan 82,24% setelah 48 jam. Berdasarkan pada parameter sitotoksisitas (CD50%) kedua plat rekonstruksi baik yang terbuat dari titanium murni maupun yang terbuat dari stainless steel tipe 316L merupakan bahan yang tidak bersifat toksik terhadap fibroblas. Kesimpulan: Kedua plat rekonstruksi baik yang terbuat dari stainless steel maupun CP titanium tidak bersifat toksik terhadap fibroblas, walaupun plat stainless steel menunjukkan level sitotoksisitas yang lebih rendah daripada titanium murni. Dengan demikian plat rekonstruksi yang terbuat dari stainless steel 316 L aman digunakan sebagai bahan untuk rekonstruksi mandibula.</dc:description>
	<dc:publisher xml:lang="en-US">Faculty of Dental Medicine, Universitas Airlangga https://fkg.unair.ac.id/en</dc:publisher>
	<dc:date>2011-03-01</dc:date>
	<dc:type>info:eu-repo/semantics/article</dc:type>
	<dc:type>info:eu-repo/semantics/publishedVersion</dc:type>
	<dc:type xml:lang="en-US">Peer-reviewed Article</dc:type>
	<dc:format>application/pdf</dc:format>
	<dc:identifier>https://e-journal.unair.ac.id/MKG/article/view/880</dc:identifier>
	<dc:identifier>10.20473/j.djmkg.v44.i1.p7-11</dc:identifier>
	<dc:source xml:lang="en-US">Dental Journal (Majalah Kedokteran Gigi); Vol. 44 No. 1 (2011): March 2011; 7-11</dc:source>
	<dc:source>2442-9740</dc:source>
	<dc:source>1978-3728</dc:source>
	<dc:language>eng</dc:language>
	<dc:relation>https://e-journal.unair.ac.id/MKG/article/view/880/664</dc:relation>
	<dc:rights xml:lang="en-US">Copyright (c) 2015 Dental Journal (Majalah Kedokteran Gigi)</dc:rights>
</oai_dc:dc>