The difference between porcelain and composite resin shear bond strength in the administration of 4% and 19.81% silane

Dental Journal (Majalah Kedokteran Gigi) · Vol. 52 No. 1 (2019) · hlm. 27–31

DOI
10.20473/j.djmkg.v52.i1.p27-31
ISSN
2442-9740, 1978-3728
Terbit
2019-03-31
Penerbit
Faculty of Dental Medicine, Universitas Airlangga https://fkg.unair.ac.id/en
Bahasa
eng

Abstrak

Background: Damage to porcelain restorations such as fractures requires a repair that can be performed either directly or indirectly. Direct repair involves directly performing restoration of fractured porcelain with a composite resin application. This technique has more advantages than indirect repair because it requires no laboratory work and can be completed during a single visit. Silane, on the other hand, has been widely used and is reported to increase porcelain and composite resin attachments during the direct repair process. Purpose: This study aimed to determine the differences in shear bond strength between porcelain and composite resin during the administering of 4% and 19.81% silane. Methods: 27 porcelain samples were divided into three groups, namely: Group A - 4% silane, Group B - 19.81% silane and Group C - no silane, prior to the application of composite resin. Each sample was tested for shear bond strength by means of Autograph and fracture analysis performed through stereomicroscope and scanning electron microscope tests. Data analysis was subsequently performed using an ANOVA test. Results: There was a significant difference between the three groups with p=0.000 (p<0.005). The lowest bond strength was found in the group without silane, while the highest was in the group with 4% silane (p<0.005). Conclusion: The use of 4% silane can produce the highest shear bond strength of porcelain and resin composite.

Kata kunci

Jaringan kolaborasi para penulis

31 penulis · 85 tautan kepenulisan bersama · 8 lintas organisasi

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • Universitas Airlangga
  • Jenderal Soedirman University
  • Royal College of Surgeons of Edinburgh
  • Afiliasi tidak diketahui
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama
Widya SaraswatiUniversitas Airlangga2
Fauziah Diajeng RetnaningsihUniversitas Airlangga2
Evri Kusumah NingtyasUniversitas Airlangga2
Sri KunartiUniversitas Airlangga2
Ketut SuarditaUniversitas Airlangga1
Irfan DwiandhonoJenderal Soedirman University1
Adioro SoetojoUniversitas Airlangga1
Febriastuti CahyaniUniversitas Airlangga1
Cecilia G.J. LunardhiUniversitas Airlangga1
Adeline Jovita TambayongUniversitas Airlangga1
Debby Fauziah SuryaniUniversitas Airlangga1
Andrie Handy KusumaUniversitas Airlangga1
Rini Devijanti RidwanAfiliasi tidak diketahui1
Kuntaman KuntamanUniversitas Airlangga1
Nur DianawatiUniversitas Airlangga1
Wahyu SetyariniUniversitas Airlangga1
Ari SubiyantoUniversitas Airlangga1
Rendy PopyandraUniversitas Airlangga1
Michael Golden KurniawanUniversitas Airlangga1
Agus SubiwahjudiUniversitas Airlangga1
Riyan Iman MarsetyoUniversitas Airlangga1
Sagita Putri AndyningtyasUniversitas Airlangga1
Chonny Salsabilla ZamrutizahraUniversitas Airlangga1
Ivan Nur FadelaUniversitas Airlangga1
Tengku Natasha Eleena binti Tengku Ahmad NoorRoyal College of Surgeons of Edinburgh1
SukatonUniversitas Airlangga1
Yashinta RamadhintaUniversitas Airlangga1
Tiffany Josephine HidayatUniversitas Airlangga1

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OAI-PMH (metadata jurnal) https://e-journal.unair.ac.id/MKG/oai, pertama di-harvest 8 Nov 2026, terakhir terlihat 8 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/  http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
	<dc:title xml:lang="en-US">The difference between porcelain and composite resin shear bond strength in the administration of 4% and 19.81% silane</dc:title>
	<dc:creator>Widjiastuti, Ira</dc:creator>
	<dc:creator>Junaedi, Dwina Rahmawati</dc:creator>
	<dc:creator>Effendy, Ruslan</dc:creator>
	<dc:subject xml:lang="en-US">porcelain repair</dc:subject>
	<dc:subject xml:lang="en-US">shear bond strength</dc:subject>
	<dc:subject xml:lang="en-US">silane</dc:subject>
	<dc:description xml:lang="en-US">Background: Damage to porcelain restorations such as fractures requires a repair that can be performed either directly or indirectly. Direct repair involves directly performing restoration of fractured porcelain with a composite resin application. This technique has more advantages than indirect repair because it requires no laboratory work and can be completed during a single visit. Silane, on the other hand, has been widely used and is reported to increase porcelain and composite resin attachments during the direct repair process. Purpose: This study aimed to determine the differences in shear bond strength between porcelain and composite resin during the administering of 4% and 19.81% silane. Methods: 27 porcelain samples were divided into three groups, namely: Group A - 4% silane, Group B - 19.81% silane and Group C - no silane, prior to the application of composite resin. Each sample was tested for shear bond strength by means of Autograph and fracture analysis performed through stereomicroscope and scanning electron microscope tests. Data analysis was subsequently performed using an ANOVA test. Results: There was a significant difference between the three groups with p=0.000 (p&amp;lt;0.005). The lowest bond strength was found in the group without silane, while the highest was in the group with 4% silane (p&amp;lt;0.005). Conclusion: The use of 4% silane can produce the highest shear bond strength of porcelain and resin composite.</dc:description>
	<dc:publisher xml:lang="en-US">Faculty of Dental Medicine, Universitas Airlangga https://fkg.unair.ac.id/en</dc:publisher>
	<dc:date>2019-03-31</dc:date>
	<dc:type>info:eu-repo/semantics/article</dc:type>
	<dc:type>info:eu-repo/semantics/publishedVersion</dc:type>
	<dc:type xml:lang="en-US">Peer-reviewed Article</dc:type>
	<dc:format>application/pdf</dc:format>
	<dc:identifier>https://e-journal.unair.ac.id/MKG/article/view/12419</dc:identifier>
	<dc:identifier>10.20473/j.djmkg.v52.i1.p27-31</dc:identifier>
	<dc:source xml:lang="en-US">Dental Journal (Majalah Kedokteran Gigi); Vol. 52 No. 1 (2019): March 2019; 27-31</dc:source>
	<dc:source>2442-9740</dc:source>
	<dc:source>1978-3728</dc:source>
	<dc:language>eng</dc:language>
	<dc:relation>https://e-journal.unair.ac.id/MKG/article/view/12419/8193</dc:relation>
	<dc:rights xml:lang="en-US">Copyright (c) 2019 Dental Journal (Majalah Kedokteran Gigi)</dc:rights>
</oai_dc:dc>