The compressive strength and static biodegradation rate of chitosan-gelatin limestone-based carbonate hydroxyapatite composite scaffold

Dental Journal (Majalah Kedokteran Gigi) · Vol. 56 No. 3 (2023) · hlm. 160–165

DOI
10.20473/j.djmkg.v56.i3.p160-165
ISSN
2442-9740, 1978-3728
Terbit
2023-06-09
Penerbit
Faculty of Dental Medicine, Universitas Airlangga https://fkg.unair.ac.id/en
Bahasa
eng
Lisensi
creativecommons.org/licenses/by-sa/4.0

Abstrak

Background: One of the main components in tissue engineering is the scaffold, which may serve as a medium to support cell and tissue growth. Scaffolds must have good compressive strength and controlled biodegradability to show biological activities while treating bone defects. This study uses Chitosan-gelatin (C–G) with good flexibility and elasticity and high-strength carbonate hydroxyapatite (CHA), which may be the ideal scaffold for tissue engineering. Purpose: To analyze the compressive strength and static biodegradation rate within various ratios of C–G and CHA (C–G:CHA) scaffold as a requirement for bone tissue engineering. Methods: The scaffold is synthesized from C–G:CHA with three ratio variations, which are 40:60, 30:70, and 20:80 (weight for weight [w/w]), made with a freeze-drying method. The compressive strengths are then tested. The biodegradation rate is tested by soaking the scaffold in simulated body fluid for 1, 3, 7, 14, and 21 days. Data are analyzed with a one-way ANOVA parametric test. Results: The compressive strength of each ratio of C–G:CHA scaffold 40:60 (w/w), 30:70 (w/w), and 20:80 (w/w), consecutively, are 4.2 Megapascals (MPa), 3.3 MPa, 2.2 MPa, and there are no significant differences with the p= 0.069 (p>0.05). The static biodegradation percentage after 21 days on each ratio variation of C–G:CHA scaffold 40:60 (w/w), 30:70 (w/w), and 20:80 (w/w) is 25.98%, 24.67%, and 20.64%. One-way ANOVA Welch test shows the result of the p-value as p<0.05. Conclusion: The compressive strength and static biodegradation of the C–G:CHA scaffold with ratio variations of 40:60 (w/w), 30:70 (w/w), and 20:80(w/w) fulfilled the requirements as a scaffold for bone tissue engineering.

Kata kunci

Jaringan kolaborasi para penulis

40 penulis · 107 tautan kepenulisan bersama · 24 lintas organisasi · menampilkan 40 yang paling banyak terhubung

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • Universitas Airlangga
  • Universitas Hang Tuah
  • University of Technology Malaysia
  • Universitas Indo Global Mandiri
  • Hasanuddin University
  • Afiliasi tidak diketahui
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama
OctarinaAfiliasi tidak diketahui3
Muhammad Riza Hafidz BahtiarUniversitas Airlangga3
Rizki Fauziah SalmaUniversitas Airlangga3
Ajeng Putri MeyrantiUniversitas Airlangga3
Maretaningtias Dwi ArianiUniversitas Airlangga2
Intan Fajrin ArsyadaUniversitas Airlangga2
Muhammad Fadhiel AlieUniversitas Indo Global Mandiri1
Imelda SaluzaUniversitas Indo Global Mandiri1
Sularsih SularsihUniversitas Hang Tuah1
Coen Pramono DUniversitas Airlangga1
Siswanto SiswantoHasanuddin University1
Retna ApsariUniversitas Airlangga1
Noriah BidinUniversity of Technology Malaysia1
Tokok AdiartoUniversitas Airlangga1
Ajeng Kartika Sri WardaniUniversitas Airlangga1
Sri YogyartiUniversitas Airlangga1
Irmawati IrmawatiUniversitas Airlangga1
Intan NirwanaUniversitas Airlangga1
Ajeng AnggraeniUniversitas Airlangga1
David DavidUniversitas Airlangga1
Agni Febrina PargaputriUniversitas Hang Tuah1
Retno IndrawatiUniversitas Airlangga1
Ariyati Retno PratiwiUniversitas Airlangga1
Istiati SoepribadiUniversitas Airlangga1
Retno Pudji RahayuUniversitas Airlangga1
Fitria RahmitasariUniversitas Hang Tuah1
Indah Liatiana KriswandiniAfiliasi tidak diketahui1
Nadia KartikasariUniversitas Airlangga1
Indah Listiana KriswandiniUniversitas Airlangga1
Moh. Basroni RizalUniversitas Hang Tuah1

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OAI-PMH (metadata jurnal) https://e-journal.unair.ac.id/MKG/oai, pertama di-harvest 8 Nov 2026, terakhir terlihat 8 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/  http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
	<dc:title xml:lang="en-US">The compressive strength and static biodegradation rate of chitosan-gelatin limestone-based carbonate hydroxyapatite composite scaffold</dc:title>
	<dc:creator>Rianti, Devi</dc:creator>
	<dc:creator>Purnamasari, Alqomariyah Eka</dc:creator>
	<dc:creator>Putri, Rifayinqa Ruyani </dc:creator>
	<dc:creator>Salsabilla, Noor Zain</dc:creator>
	<dc:creator>Faradillah</dc:creator>
	<dc:creator>Munadziroh, Elly</dc:creator>
	<dc:creator>Agustantina, Titien Hary</dc:creator>
	<dc:creator>Meizarini, Asti</dc:creator>
	<dc:creator>Yuliati, Anita </dc:creator>
	<dc:creator>Syahrom, Ardiyansyah</dc:creator>
	<dc:subject xml:lang="en-US">biodegradation</dc:subject>
	<dc:subject xml:lang="en-US">compressive strength</dc:subject>
	<dc:subject xml:lang="en-US">medicine</dc:subject>
	<dc:subject xml:lang="en-US">scaffold</dc:subject>
	<dc:description xml:lang="en-US"> Background: One of the main components in tissue engineering is the scaffold, which may serve as a medium to support cell and tissue growth. Scaffolds must have good compressive strength and controlled biodegradability to show biological activities while treating bone defects. This study uses Chitosan-gelatin (C–G) with good flexibility and elasticity and high-strength carbonate hydroxyapatite (CHA), which may be the ideal scaffold for tissue engineering. Purpose: To analyze the compressive strength and static biodegradation rate within various ratios of C–G and CHA (C–G:CHA) scaffold as a requirement for bone tissue engineering. Methods: The scaffold is synthesized from C–G:CHA with three ratio variations, which are 40:60, 30:70, and 20:80 (weight for weight [w/w]), made with a freeze-drying method. The compressive strengths are then tested. The biodegradation rate is tested by soaking the scaffold in simulated body fluid for 1, 3, 7, 14, and 21 days. Data are analyzed with a one-way ANOVA parametric test. Results: The compressive strength of each ratio of C–G:CHA scaffold 40:60 (w/w), 30:70 (w/w), and 20:80 (w/w), consecutively, are 4.2 Megapascals (MPa), 3.3 MPa, 2.2 MPa, and there are no significant differences with the p= 0.069 (p&amp;gt;0.05). The static biodegradation percentage after 21 days on each ratio variation of C–G:CHA scaffold 40:60 (w/w), 30:70 (w/w), and 20:80 (w/w) is 25.98%, 24.67%, and 20.64%. One-way ANOVA Welch test shows the result of the p-value as p&amp;lt;0.05. Conclusion: The compressive strength and static biodegradation of the C–G:CHA scaffold with ratio variations of 40:60 (w/w), 30:70 (w/w), and 20:80(w/w) fulfilled the requirements as a scaffold for bone tissue engineering. </dc:description>
	<dc:publisher xml:lang="en-US">Faculty of Dental Medicine, Universitas Airlangga https://fkg.unair.ac.id/en</dc:publisher>
	<dc:date>2023-06-09</dc:date>
	<dc:type>info:eu-repo/semantics/article</dc:type>
	<dc:type>info:eu-repo/semantics/publishedVersion</dc:type>
	<dc:format>application/pdf</dc:format>
	<dc:format>text/xml</dc:format>
	<dc:identifier>https://e-journal.unair.ac.id/MKG/article/view/39676</dc:identifier>
	<dc:identifier>10.20473/j.djmkg.v56.i3.p160-165</dc:identifier>
	<dc:source xml:lang="en-US">Dental Journal (Majalah Kedokteran Gigi); Vol. 56 No. 3 (2023): September; 160-165</dc:source>
	<dc:source>2442-9740</dc:source>
	<dc:source>1978-3728</dc:source>
	<dc:language>eng</dc:language>
	<dc:relation>https://e-journal.unair.ac.id/MKG/article/view/39676/24933</dc:relation>
	<dc:relation>https://e-journal.unair.ac.id/MKG/article/view/39676/39843</dc:relation>
	<dc:rights xml:lang="en-US">Copyright (c) 2023 Dental Journal</dc:rights>
	<dc:rights xml:lang="en-US">https://creativecommons.org/licenses/by-sa/4.0</dc:rights>
</oai_dc:dc>