Melola Discovery

← Melola Discovery

Akses terbuka Jurnal SINTA 1

Phytochemical-Mediated Green Synthesis of ZnO/Hydroxyapatite Nanocomposite from Shallot Peel Extract and Seashell Waste for Visible-Light-Assisted Photocatalytic Degradation of Remazol Red RB Textile Dye

Bulletin of Chemical Reaction Engineering & Catalysis · Vol. ume (2026) · hlm. 1018–1031

DOI
10.9767/bcrec.20812
ISSN
1978-2993
Terbit
2026-12-26
Penerbit
Masyarakat Katalis Indonesia - Indonesian Catalyst Society (MKICS)
Bahasa
eng
Lisensi
creativecommons.org/licenses/by-sa/4.0

Abstrak

Textile wastewater containing persistent synthetic dyes poses significant environmental concerns due to the toxicity and low biodegradability of these dyes. This study developed a sustainable ZnO/hydroxyapatite (ZnO/HA) nanocomposite photocatalyst using shallot peel extract and seashell waste as renewable precursors for the visible-light-assisted degradation of Remazol Red RB (RRRB) dye. ZnO nanoparticles were synthesized through a phytochemical-mediated route using aqueous shallot peel extract, while hydroxyapatite was obtained from seashell waste. The resulting ZnO/HA nanocomposite, prepared at a mass ratio of 1:2.5, was characterized using XRD, FTIR, SEM-EDX, and point-of-zero-charge analysis. The effects of catalyst dosage, solution pH, initial dye concentration, and irradiation time on RRRB degradation were investigated under a 50 W visible-light source. XRD analysis confirmed the coexistence of crystalline ZnO and hydroxyapatite phases, with an average crystallite size of 24.80 nm and crystallinity of 80.20%. The highest degradation efficiency obtained in the investigated conditions was 95.85% for 10 mg/L RRRB in 250 mL solution at pH of 6 using 1.0 g of ZnO/HA after 150 min irradiation. Under identical conditions, pristine ZnO achieved 93.40% degradation. The modest improvement indicates that the contribution of hydroxyapatite was primarily associated with surface adsorption, dispersion of ZnO, and increased pollutant–catalyst interaction rather than a demonstrated modification of the ZnO band structure. Because UV–Vis diffuse reflectance and catalyst-reusability measurements were not performed, changes in optical bandgap and long-term catalyst stability could not be experimentally established. Nevertheless, the results demonstrate the feasibility of utilizing two locally available biowaste resources to prepare a ZnO/HA material for visible-light-assisted dye treatment. Copyright © 2026 by Authors, Published by BCREC Publishing Group. This is an open access article under the CC BY-SA License (https://creativecommons.org/licenses/by-sa/4.0).

Kata kunci

Jaringan kolaborasi para penulis

13 penulis · 38 tautan kepenulisan bersama · 12 lintas organisasi

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • Universitas Pendidikan Ganesha
  • Udayana University
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama
I Gusti Lanang WiratmaUniversitas Pendidikan Ganesha2
I Gede MahardikaUdayana University2
I Wayan Budiarsa SuyasaUdayana University2
Iryanti Eka SuprihatinUdayana University2
Dewa Komang DarmayasaUniversitas Pendidikan Ganesha2
I Wayan SujaUniversitas Pendidikan Ganesha2
Ni Made WiratiniUniversitas Pendidikan Ganesha2
Ni Luh Putu Ananda SaraswatiUniversitas Pendidikan Ganesha2
I Ketut SudianaUniversitas Pendidikan Ganesha2
I Made GunamanthaUniversitas Pendidikan Ganesha1

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OAI-PMH (metadata jurnal) https://journal.bcrec.id/index.php/bcrec/oai, pertama di-harvest 8 Nov 2026, terakhir terlihat 8 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/  http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
	<dc:title xml:lang="en-US">Phytochemical-Mediated Green Synthesis of ZnO/Hydroxyapatite Nanocomposite from Shallot Peel Extract and Seashell Waste for Visible-Light-Assisted Photocatalytic Degradation of Remazol Red RB Textile Dye</dc:title>
	<dc:creator>Sukarta, I Nyoman</dc:creator>
	<dc:creator>Sastrawidana, I Dewa Ketut</dc:creator>
	<dc:creator>Rachmawati, Dewi Oktofa</dc:creator>
	<dc:subject xml:lang="en-US">Green synthesis; hydroxyapatite; remazol red RB; visible-light photocatalysis; ZnO/HA nanocomposite</dc:subject>
	<dc:description xml:lang="en-US">Textile wastewater containing persistent synthetic dyes poses significant environmental concerns due to the toxicity and low biodegradability of these dyes. This study developed a sustainable ZnO/hydroxyapatite (ZnO/HA) nanocomposite photocatalyst using shallot peel extract and seashell waste as renewable precursors for the visible-light-assisted degradation of Remazol Red RB (RRRB) dye. ZnO nanoparticles were synthesized through a phytochemical-mediated route using aqueous shallot peel extract, while hydroxyapatite was obtained from seashell waste. The resulting ZnO/HA nanocomposite, prepared at a mass ratio of 1:2.5, was characterized using XRD, FTIR, SEM-EDX, and point-of-zero-charge analysis. The effects of catalyst dosage, solution pH, initial dye concentration, and irradiation time on RRRB degradation were investigated under a 50 W visible-light source. XRD analysis confirmed the coexistence of crystalline ZnO and hydroxyapatite phases, with an average crystallite size of 24.80 nm and crystallinity of 80.20%. The highest degradation efficiency obtained in the investigated conditions was 95.85% for 10 mg/L RRRB in 250 mL solution at pH of 6 using 1.0 g of ZnO/HA after 150 min irradiation. Under identical conditions, pristine ZnO achieved 93.40% degradation. The modest improvement indicates that the contribution of hydroxyapatite was primarily associated with surface adsorption, dispersion of ZnO, and increased pollutant–catalyst interaction rather than a demonstrated modification of the ZnO band structure. Because UV–Vis diffuse reflectance and catalyst-reusability measurements were not performed, changes in optical bandgap and long-term catalyst stability could not be experimentally established. Nevertheless, the results demonstrate the feasibility of utilizing two locally available biowaste resources to prepare a ZnO/HA material for visible-light-assisted dye treatment. Copyright © 2026 by Authors, Published by BCREC Publishing Group. This is an open access article under the CC BY-SA License (https://creativecommons.org/licenses/by-sa/4.0).</dc:description>
	<dc:publisher xml:lang="en-US">Masyarakat Katalis Indonesia - Indonesian Catalyst Society (MKICS)</dc:publisher>
	<dc:date>2026-12-26</dc:date>
	<dc:type>info:eu-repo/semantics/article</dc:type>
	<dc:type>info:eu-repo/semantics/publishedVersion</dc:type>
	<dc:type xml:lang="en-US"></dc:type>
	<dc:format>application/pdf</dc:format>
	<dc:identifier>https://journal.bcrec.id/index.php/bcrec/article/view/20812</dc:identifier>
	<dc:identifier>10.9767/bcrec.20812</dc:identifier>
	<dc:source xml:lang="en-US">Bulletin of Chemical Reaction Engineering &amp; Catalysis; 2026: BCREC Volume 21 Issue 4 Year 2026 (December 2026); 1018-1031</dc:source>
	<dc:source>1978-2993</dc:source>
	<dc:language>eng</dc:language>
	<dc:relation>https://journal.bcrec.id/index.php/bcrec/article/view/20812/10014</dc:relation>
	<dc:relation>https://journal.bcrec.id/index.php/bcrec/article/downloadSuppFile/20812/6579</dc:relation>
	<dc:rights xml:lang="en-US">Copyright (c) 2026 by Authors, Published by BCREC Publishing Group</dc:rights>
	<dc:rights xml:lang="en-US">https://creativecommons.org/licenses/by-sa/4.0</dc:rights>
</oai_dc:dc>