Study of Micro-hardness of High-Speed W9Mo4Co8 Steel Plates in Pendulum Grinding by Abrasive Wheel Periphery

Journal of Engineering and Technological Sciences · Vol. 49 No. 3 (2017) · hlm. 291–307

DOI
10.5614/j.eng.technol.sci.2017.49.3.1
ISSN
2338-5502, 2337-5779
Terbit
2017-08-31
Penerbit
Directorate for Research and Community Services, Institut Teknologi Bandung
Bahasa
eng

Abstrak

In cutting tool assembly, grinding is the most important technological step of the finishing treatment, largely determining the workmanship. An increase of micro-hardness after grinding relative to the original one indicates the dominant role of abrasive tool force impact on the ground surface. A decrease, in contrast, evidences a significant softening under the influence of heat source. This research based on nonparametric statistics to predict the effect of wheel characteristics with abrasives 25A, 92A/25A, 34A, 5A, EKE, 5NQ, TGX, 5SG and with graininess 46 (F46), 60 (F60), 80 with different porosities (structure numbers 6-12), and the expected measures of position and dispersion on the micro-hardness of the surface of a high-speed cutting plate (HSCP) made of W9Mo4Co8 steel. It was found that grinding this HSCP by wheels 5NQ46I6VS3, 5SG46K12VXP, 5SG60K12VXP, 5SG46I12VXP, 25AF46M12V5"“PO, 25AF46M12V5"“PO3, 25АF46M10V5"“PO, 25AF46M10V5"“PO3, 25AF46K10V5"“PO3, 25AF60M10V5"“PO3, 25AF46L10V5"“KF35, EKE46K3V, 92A/25AF46L6V20 occurred without surface softening for 50% of the details from the operating batch.

Kata kunci

Jaringan kolaborasi para penulis

4 penulis · 4 tautan kepenulisan bersama

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • Irkutsk National Research Technical University
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama
Nguyen Manh TiemIrkutsk National Research Technical University1
Nguyen Van LeIrkutsk National Research Technical University1

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OAI-PMH (metadata jurnal) https://journals.itb.ac.id/index.php/jets/oai, pertama di-harvest 9 Nov 2026, terakhir terlihat 22 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/  http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
	<dc:title xml:lang="en-US">Study of Micro-hardness of High-Speed W9Mo4Co8 Steel Plates in Pendulum Grinding by Abrasive Wheel Periphery</dc:title>
	<dc:creator>Soler, Yakov Iosifovich</dc:creator>
	<dc:creator>Nguyen, Van Canh</dc:creator>
	<dc:subject xml:lang="en-US">abrasive wheels</dc:subject>
	<dc:subject xml:lang="en-US">grinding</dc:subject>
	<dc:subject xml:lang="en-US">measure of position and dispersion</dc:subject>
	<dc:subject xml:lang="en-US">micro-hardness</dc:subject>
	<dc:subject xml:lang="en-US">stability of the process</dc:subject>
	<dc:subject xml:lang="en-US">statistics.</dc:subject>
	<dc:description xml:lang="en-US">In cutting tool assembly, grinding is the most important technological step of the finishing treatment, largely determining the workmanship. An increase of micro-hardness after grinding relative to the original one indicates the dominant role of abrasive tool force impact on the ground surface. A decrease, in contrast, evidences a significant softening under the influence of heat source. This research based on nonparametric statistics to predict the effect of wheel characteristics with abrasives 25A, 92A/25A, 34A, 5A, EKE, 5NQ, TGX, 5SG and with graininess 46 (F46), 60 (F60), 80 with different porosities (structure numbers 6-12), and the expected measures of position and dispersion on the micro-hardness of the surface of a high-speed cutting plate (HSCP) made of W9Mo4Co8 steel. It was found that grinding this HSCP by wheels 5NQ46I6VS3, 5SG46K12VXP, 5SG60K12VXP, 5SG46I12VXP, 25AF46M12V5"“PO, 25AF46M12V5"“PO3, 25АF46M10V5"“PO, 25AF46M10V5"“PO3, 25AF46K10V5"“PO3, 25AF60M10V5"“PO3, 25AF46L10V5"“KF35, EKE46K3V, 92A/25AF46L6V20 occurred without surface softening for 50% of the details from the operating batch.</dc:description>
	<dc:publisher xml:lang="en-US">Directorate for Research and Community Services, Institut Teknologi Bandung</dc:publisher>
	<dc:date>2017-08-31</dc:date>
	<dc:type>info:eu-repo/semantics/article</dc:type>
	<dc:type>info:eu-repo/semantics/publishedVersion</dc:type>
	<dc:format>application/pdf</dc:format>
	<dc:identifier>https://journals.itb.ac.id/index.php/jets/article/view/3221</dc:identifier>
	<dc:identifier>10.5614/j.eng.technol.sci.2017.49.3.1</dc:identifier>
	<dc:source xml:lang="en-US">Journal of Engineering and Technological Sciences; Vol. 49 No. 3 (2017); 291-307</dc:source>
	<dc:source>2338-5502</dc:source>
	<dc:source>2337-5779</dc:source>
	<dc:source>10.5614/j.eng.technol.sci.2017.49.3</dc:source>
	<dc:language>eng</dc:language>
	<dc:relation>https://journals.itb.ac.id/index.php/jets/article/view/3221/2959</dc:relation>
</oai_dc:dc>