Abstrak

This work has investigate conditions which allow pitting corrosion of carbon steel in acetate buffered test solutions of pH 3.82, 4.12, 5.12 and 6.12, 0.2 M NaOAc and standard brine solutions, all of which contains 100 mg/L sodium bicarbonate and saturated with CO2. Corrosion rates is determined by corrosion wheel and corrosion bubble tests, while surface morphology is observed by electron microscopy (SEM) and metallographic optical microscopy, whereas surface deterioration as well as corroded lattice structure of the steel is monitored through measurements by X-ray Diffraction (XRD) patterns. The X-ray Diffraction Patterns of corroded carbon steel in any of the above test solutions exhibit a decrease in relative intensity of 110 and 200 lattice planes and an increase in the 211 lattice plane. The extent of decrease of the diffracted X-ray intensities increases with the increase in the percentage of corroded carbon steel coupon weight loss. This might reflect a selective dissolution of iron atoms situated in both lattice planes. It is suspected that this observation is due to the fact that 211 lattice plane has the smallest percentage of atomic occupancy among the three, thus it might have the greatest chance to be inserted with carbon atoms which in turn gives a protective effect toward iron atoms against further dissolution. Although, the corrosion process starts from the surface phase, this experiment reveals that X-ray diffraction pattern of the three lattice planes could be employed as some sort of carbon steel corrosion indicator. Consequently, corrosion inhibitor performance could be deduced from its ability to maintain diffraction pattern of the initial carbon steel specimen.

Jaringan kolaborasi para penulis

19 penulis · 52 tautan kepenulisan bersama · 14 lintas organisasi

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • Bandung Institute of Technology
  • National Research and Innovation Agency
  • Yogyakarta State University
  • State University of Semarang
  • Tadulako University
  • Universitas Sembilanbelas November Kolaka
  • Afiliasi tidak diketahui
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama
I Made ArcanaBandung Institute of Technology4
Deana WahyuningrumBandung Institute of Technology4
Cynthia Linaya RadimanBandung Institute of Technology4
Enny RatnaningsihBandung Institute of Technology3
Sadijah AchmadBandung Institute of Technology3
Sun Theo Constan Lotebulo NdruruNational Research and Innovation Agency2
Eli RohaetiYogyakarta State University2
Supartono SupartonoState University of Semarang1
Buchari BuchariAfiliasi tidak diketahui1
Yana Maolana SyahBandung Institute of Technology1
Siang Tandi GonggoTadulako University1
Marlina MarlinaAfiliasi tidak diketahui1
Muhammad MasykuriBandung Institute of Technology1
Fitri Widya HartantiBandung Institute of Technology1
Muhamad Jalil BaariUniversitas Sembilanbelas November Kolaka1

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OAI-PMH (metadata jurnal) https://journals.itb.ac.id/index.php/jmfs/oai, pertama di-harvest 9 Nov 2026, terakhir terlihat 16 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/  http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
	<dc:title xml:lang="en-US">Pelarutan Besi Selektif pada Korosi Baja Karbon dalam Larutan Buffer Asetat, Natrium Bikarbonat - CO2 Jenuh</dc:title>
	<dc:creator>Bundjali, Bunbun</dc:creator>
	<dc:creator>Surdia, N. M.</dc:creator>
	<dc:creator>Liang, Oei Ban</dc:creator>
	<dc:creator>Ariwahjoedi, Bambang</dc:creator>
	<dc:description xml:lang="en-US"> This work has investigate conditions which allow pitting corrosion of carbon steel in acetate buffered test solutions of pH 3.82, 4.12, 5.12 and 6.12, 0.2 M NaOAc and standard brine solutions, all of which contains 100 mg/L sodium bicarbonate and saturated with CO2. Corrosion rates is determined by corrosion wheel and corrosion bubble tests, while surface morphology is observed by electron microscopy (SEM) and metallographic optical microscopy, whereas surface deterioration as well as corroded lattice structure of the steel is monitored through measurements by X-ray Diffraction (XRD) patterns. The X-ray Diffraction Patterns of corroded carbon steel in any of the above test solutions exhibit a decrease in relative intensity of 110 and 200 lattice planes and an increase in the 211 lattice plane. The extent of decrease of the diffracted X-ray intensities increases with the increase in the percentage of corroded carbon steel coupon weight loss. This might reflect a selective dissolution of iron atoms situated in both lattice planes. It is suspected that this observation is due to the fact that 211 lattice plane has the smallest percentage of atomic occupancy among the three, thus it might have the greatest chance to be inserted with carbon atoms which in turn gives a protective effect toward iron atoms against further dissolution. Although, the corrosion process starts from the surface phase, this experiment reveals that X-ray diffraction pattern of the three lattice planes could be employed as some sort of carbon steel corrosion indicator. Consequently, corrosion inhibitor performance could be deduced from its ability to maintain diffraction pattern of the initial carbon steel specimen.</dc:description>
	<dc:publisher xml:lang="en-US">Directorate for Research and Innovation (DRI) ITB</dc:publisher>
	<dc:date>2013-12-31</dc:date>
	<dc:type>info:eu-repo/semantics/article</dc:type>
	<dc:type>info:eu-repo/semantics/publishedVersion</dc:type>
	<dc:format>application/pdf</dc:format>
	<dc:identifier>https://journals.itb.ac.id/index.php/jmfs/article/view/295</dc:identifier>
	<dc:identifier>10.5614/itbj.sci.2006.38.2.5</dc:identifier>
	<dc:source xml:lang="en-US">Journal of Mathematical and Fundamental Sciences; Vol. 38 No. 2 (2006); 149-161</dc:source>
	<dc:source>2338-5510</dc:source>
	<dc:source>2337-5760</dc:source>
	<dc:language>eng</dc:language>
	<dc:relation>https://journals.itb.ac.id/index.php/jmfs/article/view/295/278</dc:relation>
</oai_dc:dc>