Effect of the Specimen’s Height on the Split-Tensile Strength of the Fibers Reinforced Clay-Lime-Rice Husk Ask Mixture

Journal of the Civil Engineering Forum · Vol. 10 No. 2 (2024) · hlm. 209–216

DOI
10.22146/jcef.11305
ISSN
2549-5925, 2581-1037
Terbit
2024-04-22
Penerbit
Department of Civil and Environmental Engineering, Faculty of Engineering, Universitas Gadjah Mada
Bahasa
eng

Abstrak

Various studies on the effect of specimen size on splitting tensile strength. However, geotechnical codes lack consensus regarding the recommended specimen diameter and height-to-diameter (H/D) ratio for the split tensile strength test. Hence, it is imperative to study the effect of the height-to-diameter ratio of the specimen on the outcomes of the split tensile strength test, especially for stabilized and fiber-reinforced soil. This research examines the effect of adding lime-rice husk ash and plastic fiber and the effect of specimen size on splitting tensile strength. The height of the specimen is varied, using a height-to-diameter ratio (H/D), namely 0.5, 1.0, 1.5, 2.0, and 2.5, in which the diameter is 70 mm. Two groups of specimens were prepared as stabilized clay without fibers and stabilized clay with 0.1% fibers. The lime required for stabilization is 10% of the dry weight of the soil. In this research, the lime and rice husk ash ratio was designed as 1:1. The splitting tensile strength test was carried out after the specimen was cured for seven days. The investigation indicates that the splitting tensile strength of the specimen without fibers reduces from 217 kPa to 150 kPa as the H/D ratio grows from 0.5 to 2.5. Conversely, the tensile strength of the specimen with fibers increases from 284 kPa to 357 kPa. The findings suggest that the fiber inclusion enhances the splitting tensile strength of the stabilized clay. The specimen size affects the splitting tensile strength, but the effect becomes less noticeable when the H/D ratio exceeds 2.5. From a fracture mechanism perspective, the specimen experiences mode II (shearing) due toa probable “flexural action” along its height. It remains challenging to conclude the dimensions of the test specimen or, at the very least, estimate the correction factor for the size-to-tensile strength ratio.

Kata kunci

Jaringan kolaborasi para penulis

19 penulis · 41 tautan kepenulisan bersama · 19 lintas organisasi

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • Muhammadiyah University of Yogyakarta
  • Universitas Jambi
  • Politeknik Negeri Tanah Laut
  • National Taiwan University of Science and Technology
  • Andalas University
  • Kyoto University
  • Kasetsart University
  • Organisasi lain
  • Afiliasi tidak diketahui
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama
Nurza Purwa AbiyogaUniversitas Jambi3
Muhammad AzharPoliteknik Negeri Tanah Laut3
Lia IndrianiMuhammadiyah University of Yogyakarta3
Jazaul IkhsanMuhammadiyah University of Yogyakarta2
Wilis DianaMuhammadiyah University of Yogyakarta2
Anita RahmawatiMuhammadiyah University of Yogyakarta2
Liao H.J.National Taiwan University of Science and Technology1
Rehni SetiatiAndalas University1
Ryosuke UzuokaKyoto University1
Nurul FataMuhammadiyah University of Yogyakarta1
Apiniti JotisankasaKasetsart University1
Kuo‐Hsin YangNational Taiwan University1
Ani HairaniMuhammadiyah University of Yogyakarta1
Muhammad Fikri PermanaMuhammadiyah University of Yogyakarta1
Farid Nur BahtiMuhammadiyah University of Yogyakarta1

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OAI-PMH (metadata jurnal) https://jurnal.ugm.ac.id/v3/jcef/oai, pertama di-harvest 9 Nov 2026, terakhir terlihat 16 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/  http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
	<dc:title xml:lang="en-US">Effect of the Specimen’s Height on the Split-Tensile Strength of the Fibers Reinforced Clay-Lime-Rice Husk Ask Mixture</dc:title>
	<dc:creator>Hartono, Edi</dc:creator>
	<dc:creator>Muntohar, Agus Setyo</dc:creator>
	<dc:creator>Diana, Willis</dc:creator>
	<dc:creator>Hemeto, Abd. Dzargifar</dc:creator>
	<dc:subject xml:lang="en-US">soil stabilization; lime; rice husk ash; fiber; splitting tensile strength; specimen size</dc:subject>
	<dc:description xml:lang="en-US">Various studies on the effect of specimen size on splitting tensile strength. However, geotechnical codes lack consensus regarding the recommended specimen diameter and height-to-diameter (H/D) ratio for the split tensile strength test. Hence, it is imperative to study the effect of the height-to-diameter ratio of the specimen on the outcomes of the split tensile strength test, especially for stabilized and fiber-reinforced soil. This research examines the effect of adding lime-rice husk ash and plastic fiber and the effect of specimen size on splitting tensile strength. The height of the specimen is varied, using a height-to-diameter ratio (H/D), namely 0.5, 1.0, 1.5, 2.0, and 2.5, in which the diameter is 70 mm. Two groups of specimens were prepared as stabilized clay without fibers and stabilized clay with 0.1% fibers. The lime required for stabilization is 10% of the dry weight of the soil. In this research, the lime and rice husk ash ratio was designed as 1:1. The splitting tensile strength test was carried out after the specimen was cured for seven days. The investigation indicates that the splitting tensile strength of the specimen without fibers reduces from 217 kPa to 150 kPa as the H/D ratio grows from 0.5 to 2.5. Conversely, the tensile strength of the specimen with fibers increases from 284 kPa to 357 kPa. The findings suggest that the fiber inclusion enhances the splitting tensile strength of the stabilized clay. The specimen size affects the splitting tensile strength, but the effect becomes less noticeable when the H/D ratio exceeds 2.5. From a fracture mechanism perspective, the specimen experiences mode II (shearing) due toa probable “flexural action” along its height. It remains challenging to conclude the dimensions of the test specimen or, at the very least, estimate the correction factor for the size-to-tensile strength ratio.</dc:description>
	<dc:publisher xml:lang="en-US">Department of Civil and Environmental Engineering, Faculty of Engineering, Universitas Gadjah Mada</dc:publisher>
	<dc:date>2024-04-22</dc:date>
	<dc:type>info:eu-repo/semantics/article</dc:type>
	<dc:type>info:eu-repo/semantics/publishedVersion</dc:type>
	<dc:type xml:lang="en-US">Peer-reviewed Article</dc:type>
	<dc:format>application/pdf</dc:format>
	<dc:identifier>https://jurnal.ugm.ac.id/v3/JCEF/article/view/11305</dc:identifier>
	<dc:identifier>10.22146/jcef.11305</dc:identifier>
	<dc:source xml:lang="en-US">Journal of the Civil Engineering Forum; Vol. 10 No. 2 (May 2024); 209-216</dc:source>
	<dc:source>2549-5925</dc:source>
	<dc:source>2581-1037</dc:source>
	<dc:language>eng</dc:language>
	<dc:relation>https://jurnal.ugm.ac.id/v3/JCEF/article/view/11305/4089</dc:relation>
	<dc:rights xml:lang="en-US">Copyright (c) 2024 The Author(s)</dc:rights>
</oai_dc:dc>