This research showcased the use of leftover trash as a substitute for aggregate in mortar combined with saltwater. The raw waste materials underwent analysis using X-ray fluorescence (XRF) in order to determine the component materials and crystalline phases present. The choice of Portland composite cement (PCC) was made because of its durability in a hostile environment. Seawater is used to combat the water crisis and prevent corrosion, thanks to its exceptional resistance to corrosion. The attributes of mortar were assessed in terms of its fresh characteristics (slump and flow table) as well as its mechanical properties (compressive strength, split tensile strength, flexural strength, density, and shrinkage). The findings indicate that the dried mortar waste is suitable as a patch repair material for a substrate with a strength of 20 MPa, but only when utilized in a maximum quantity of 20% and with a water-to-cement ratio of 0.3. The repaired concrete with a strength of 25 MPa did not need any waste containment and had a maximum water-to-cement ratio (W/C) of 0.3, whether combined with saltwater or tap water. The possible role of the mortar containing the dried waste was to be the species for brick and other non-structural. Additionally, the use of an alternative cementitious substance is suggested to enhance the effectiveness of the patch repair material, particularly when paired with cathodic corrosion protection in damaged concrete

Kata kunci

Jaringan kolaborasi para penulis

25 penulis · 103 tautan kepenulisan bersama · 44 lintas organisasi

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • Muhammadiyah University of Yogyakarta
  • PS Construction (Japan)
  • Universitas Gadjah Mada
  • Universitas Muhammadiyah Sumatera Barat
  • Universitas Negeri Surabaya
  • Afiliasi tidak diketahui
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama
Muhammad Sakti IsnainiMuhammadiyah University of Yogyakarta4
Devi SasmitaMuhammadiyah University of Yogyakarta4
Anisa ZulkarnainMuhammadiyah University of Yogyakarta4
Angga Jordi NouvaldiMuhammadiyah University of Yogyakarta4
Ahmad Choiry FajarMuhammadiyah University of Yogyakarta3
Allan Irnanda WijaksonoMuhammadiyah University of Yogyakarta3
Fajar Firdaus AlhudaMuhammadiyah University of Yogyakarta3
Daffa Firyal BaihaqiMuhammadiyah University of Yogyakarta3
Nadiva Syabilla Sari HendrawanMuhammadiyah University of Yogyakarta3
Muhammad Fauzan AbdillahMuhammadiyah University of Yogyakarta3
Monika Ayu Nelly KusumawatiMuhammadiyah University of Yogyakarta3
Naftali Zahra AthiraMuhammadiyah University of Yogyakarta3
Satya Putra RamadhanMuhammadiyah University of Yogyakarta3
Sausan Jilan Muthi'ah IzmaMuhammadiyah University of Yogyakarta3
Fadillawaty SalehMuhammadiyah University of Yogyakarta1
Hakas PrayudaMuhammadiyah University of Yogyakarta1
Berkat Cipta ZegaUniversitas Negeri Surabaya1
Martyana Dwi CahyatiMuhammadiyah University of Yogyakarta1

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OAI-PMH (metadata jurnal) https://publikasi.mercubuana.ac.id/index.php/sinergi/oai, pertama di-harvest 10 Nov 2026, terakhir terlihat 22 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/  http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
	<dc:title xml:lang="en-US">Engineering properties of seawater-mixed mortar with batching plant residual waste as aggregate replacement</dc:title>
	<dc:creator>Astuti, Pinta</dc:creator>
	<dc:creator>Pramana, Alfido Adhi</dc:creator>
	<dc:creator>Rafdinal, Rahmita Sari</dc:creator>
	<dc:creator>Purnama, Adhitya Yoga</dc:creator>
	<dc:creator>Arifan, Rusdi Sahla</dc:creator>
	<dc:creator>Monika, Fanny</dc:creator>
	<dc:creator>Habirun, Asiya Nurhasanah</dc:creator>
	<dc:subject xml:lang="en-US">Batching plant waste</dc:subject>
	<dc:subject xml:lang="en-US">Compressive strength</dc:subject>
	<dc:subject xml:lang="en-US">Durability</dc:subject>
	<dc:subject xml:lang="en-US">Patch repair</dc:subject>
	<dc:subject xml:lang="en-US">Seawater-mixed mortar</dc:subject>
	<dc:description xml:lang="en-US">This research showcased the use of leftover trash as a substitute for aggregate in mortar combined with saltwater. The raw waste materials underwent analysis using X-ray fluorescence (XRF) in order to determine the component materials and crystalline phases present. The choice of Portland composite cement (PCC) was made because of its durability in a hostile environment. Seawater is used to combat the water crisis and prevent corrosion, thanks to its exceptional resistance to corrosion. The attributes of mortar were assessed in terms of its fresh characteristics (slump and flow table) as well as its mechanical properties (compressive strength, split tensile strength, flexural strength, density, and shrinkage). The findings indicate that the dried mortar waste is suitable as a patch repair material for a substrate with a strength of 20 MPa, but only when utilized in a maximum quantity of 20% and with a water-to-cement ratio of 0.3. The repaired concrete with a strength of 25 MPa did not need any waste containment and had a maximum water-to-cement ratio (W/C) of 0.3, whether combined with saltwater or tap water. The possible role of the mortar containing the dried waste was to be the species for brick and other non-structural. Additionally, the use of an alternative cementitious substance is suggested to enhance the effectiveness of the patch repair material, particularly when paired with cathodic corrosion protection in damaged concrete</dc:description>
	<dc:publisher xml:lang="en-US">Universitas Mercu Buana</dc:publisher>
	<dc:date>2024-05-05</dc:date>
	<dc:type>info:eu-repo/semantics/article</dc:type>
	<dc:type>info:eu-repo/semantics/publishedVersion</dc:type>
	<dc:type xml:lang="en-US">Peer-reviewed Article</dc:type>
	<dc:format>application/pdf</dc:format>
	<dc:format>application/pdf</dc:format>
	<dc:format>application/vnd.openxmlformats-officedocument.wordprocessingml.document</dc:format>
	<dc:identifier>https://publikasi.mercubuana.ac.id/index.php/sinergi/article/view/23276</dc:identifier>
	<dc:identifier>10.22441/sinergi.2024.2.017</dc:identifier>
	<dc:source xml:lang="en-US">SINERGI; Vol. 28 No. 2 (2024); 381-394</dc:source>
	<dc:source>2460-1217</dc:source>
	<dc:source>1410-2331</dc:source>
	<dc:language>eng</dc:language>
	<dc:relation>https://publikasi.mercubuana.ac.id/index.php/sinergi/article/view/23276/8330</dc:relation>
	<dc:relation>https://publikasi.mercubuana.ac.id/index.php/sinergi/article/view/23276/11750</dc:relation>
	<dc:relation>https://publikasi.mercubuana.ac.id/index.php/sinergi/article/view/23276/11848</dc:relation>
	<dc:rights xml:lang="en-US">Copyright (c) 2024 SINERGI</dc:rights>
</oai_dc:dc>