Cellulose derivative as protection coating: Effect of nanoparticle additives on load capacity

Teknomekanik · Vol. 5 No. 2 (2022) · hlm. 90–96

DOI
10.24036/teknomekanik.v5i2.16372
ISSN
2621-8720, 2621-9980
Terbit
2022-12-15
Penerbit
Universitas Negeri Padang
Bahasa
eng
Lisensi
creativecommons.org/licenses/by/4.0

Abstrak

The cellulose derivative hydroxypropyl methylcellulose (HPMC) has recently been extensively studied and used in mechanical applications. However, the softness and susceptibility to deformation of HPMC limited its further applications. In this study, metal nanoparticles (nano-aluminum and nano-copper) and nano-metal oxide particles (nano-alumina and nano-copper oxide) were used as additives to HPMC to form a composite film with improved mechanical properties, particularly load capacity. The addition of high levels of additives provided a higher load capacity. Among the nano-additives used in the study, Cu (2 wt.%) provided the composite with the highest load capacity, improving the load capacity of pure HPMC by 250%. The surface treatment of strengthening additives is an important step. Adding specific high-strength and high-modulus metal and metal oxide additives to the soft HPMC matrix can effectively improve the load-bearing capacity of the composite material. This study proposes a simple evaluation method for the load-bearing capability of the coating as well.

Kata kunci

Jaringan kolaborasi para penulis

15 penulis · 52 tautan kepenulisan bersama · 38 lintas organisasi

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • National Cheng Kung University
  • Universitas Negeri Padang
  • Andalas University
  • National Research and Innovation Agency
  • Universidade Federal do Rio Grande do Norte
  • Quaid-e-Awam University of Engineering, Science and Technology
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama
Dieter RahmadiawanNational Cheng Kung University3
Chia-Feng HsiehNational Cheng Kung University1
Wei-Ting ZhuangNational Cheng Kung University1
Budi SyahriUniversitas Negeri Padang1
Yolli FernandaUniversitas Negeri Padang1
Irzal IrzalUniversitas Negeri Padang1
Eko IndrawanUniversitas Negeri Padang1
Hairul AbralAndalas University1
Imtiaz Ali LaghariQuaid-e-Awam University of Engineering, Science and Technology1
Thiago F. SantosUniversidade Federal do Rio Grande do Norte1
Tio BaskaraAndalas University1
Eni SugiartiNational Research and Innovation Agency1
Ahmad Novi MusliminNational Research and Innovation Agency1

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OAI-PMH (metadata jurnal) http://teknomekanik.ppj.unp.ac.id/index.php/teknomekanik/oai, pertama di-harvest 10 Nov 2026, terakhir terlihat 10 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/  http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
	<dc:title xml:lang="en">Cellulose derivative as protection coating: Effect of nanoparticle additives on load capacity</dc:title>
	<dc:creator xml:lang="en">Shi, Shih-Chen</dc:creator>
	<dc:creator xml:lang="en">Tsai, Xiao-Ning</dc:creator>
	<dc:subject xml:lang="en">Load capacity</dc:subject>
	<dc:subject xml:lang="en">Nanoparticle additive</dc:subject>
	<dc:subject xml:lang="en">Cellulose composite</dc:subject>
	<dc:subject xml:lang="en">Coating</dc:subject>
	<dc:description xml:lang="en">The cellulose derivative hydroxypropyl methylcellulose (HPMC) has recently been extensively studied and used in mechanical applications. However, the softness and susceptibility to deformation of HPMC limited its further applications. In this study, metal nanoparticles (nano-aluminum and nano-copper) and nano-metal oxide particles (nano-alumina and nano-copper oxide) were used as additives to HPMC to form a composite film with improved mechanical properties, particularly load capacity. The addition of high levels of additives provided a higher load capacity. Among the nano-additives used in the study, Cu (2 wt.%) provided the composite with the highest load capacity, improving the load capacity of pure HPMC by 250%.&amp;nbsp;&amp;nbsp; The surface treatment of strengthening additives is an important step. Adding specific high-strength and high-modulus metal and metal oxide additives to the soft HPMC matrix can effectively improve the load-bearing capacity of the composite material. This study proposes a simple evaluation method for the load-bearing capability of the coating as well.</dc:description>
	<dc:publisher xml:lang="en">Universitas Negeri Padang</dc:publisher>
	<dc:date>2022-12-15</dc:date>
	<dc:type>info:eu-repo/semantics/article</dc:type>
	<dc:type>info:eu-repo/semantics/publishedVersion</dc:type>
	<dc:format>application/pdf</dc:format>
	<dc:identifier>http://teknomekanik.ppj.unp.ac.id/index.php/teknomekanik/article/view/163</dc:identifier>
	<dc:identifier>10.24036/teknomekanik.v5i2.16372</dc:identifier>
	<dc:source xml:lang="en">Teknomekanik; Vol. 5 No. 2 (2022): Regular Issue; 90-96</dc:source>
	<dc:source>2621-8720</dc:source>
	<dc:source>2621-9980</dc:source>
	<dc:language>eng</dc:language>
	<dc:relation>http://teknomekanik.ppj.unp.ac.id/index.php/teknomekanik/article/view/163/130</dc:relation>
	<dc:rights xml:lang="en">Copyright (c) 2022 Shih-Chen Shi (Author)</dc:rights>
	<dc:rights xml:lang="en">http://creativecommons.org/licenses/by/4.0</dc:rights>
</oai_dc:dc>