Characteristics of sisal-epoxy composite boards with sodium chloride-treated fibers at different treatment temperatures

Teknomekanik · Vol. 8 No. 1 (2025) · hlm. 38–51

DOI
10.24036/teknomekanik.v8i1.35572
ISSN
2621-8720, 2621-9980
Terbit
2025-06-30
Penerbit
Universitas Negeri Padang
Bahasa
eng
Lisensi
creativecommons.org/licenses/by/4.0

Abstrak

The growing environmental concerns associated with synthetic fibers have led to the increased adoption of bio-fibers as reinforcements in polymer composites. Sodium chloride (NaCl) is explored as a fiber treatment agent to enhance the adhesion between fibers and the matrix. The study aims to evaluate the effects of NaCl treatment on the characteristics of sisal fiber-epoxy composite boards. A completely randomized design was applied with three factors: treatment temperature (25 °C and 100 °C), NaCl concentration (1, 3, and 5 wt%), and composite board density (0.40, 0.60, and 0.80 g/cm³). Sisal fibers were soaked in NaCl solutions for one hour, rinsed, dried, and manually blended with epoxy at a ratio of 80:20 wt%. Composite board properties were observed according to the standards of JIS-A-5908, Fourier Transform Infrared Spectroscopy (FTIR), and Scanning Electron Microscopy (SEM). Results indicated that increasing the NaCl concentration and treatment temperature significantly improved the properties of the composite board. The optimal parameters (5wt% NaCl, 100 °C, 0.80g/cm³) yielded a modulus of elasticity of 4.59±0.26 GPa, modulus of rupture of 18.88±0.03 MPa, and internal bond strength of 3.92±0.18 MPa, representing increases of 200.32%, 130.65%, and 218.70%, respectively. Thickness swelling decreased to 2.13±0.43% (48.14%) and water absorption to 8.95±0.05% (32.25%). These findings confirm that NaCl treatment is an eco-friendly method to enhance the mechanical strength and moisture resistance of biofiber composites. It also supports the development of high-performance composite boards.

Kata kunci

Jaringan kolaborasi para penulis

27 penulis · 74 tautan kepenulisan bersama · 34 lintas organisasi

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • State University of Malang
  • University of Brawijaya
  • Universiti Malaysia Perlis
  • University of Technology Malaysia
  • Andalas University
  • Universitas Negeri Padang
  • Saveetha University
  • Afiliasi tidak diketahui
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama
Yenny RisjaniUniversity of Brawijaya2
Andoko AndokoState University of Malang2
Anni FaridahUniversitas Negeri Padang2
Daimon SyukriAndalas University2
Joseph Selvi BinojSaveetha University2
Fajar NusantaraState University of Malang2
Ulfieda Anwar UlhaqState University of Malang2
Komarudin KomarudinState University of Malang2
Maykel ManawanAfiliasi tidak diketahui1
Femiana GapsariUniversity of Brawijaya1
Rifqi Ryandi Dwi AnantoState University of Malang1
Tuan Amran Tuan AbdullahUniversity of Technology Malaysia1
Uzfi Helmi ZamzamiState University of Malang1
Prihanto TrihutomoState University of Malang1
Asus Maizar SHUniversity of Brawijaya1
Ita Fitria SUniversity of Brawijaya1
Rifka Rimbi AnggrainiUniversity of Brawijaya1
Asep Awaludin PrihantoUniversity of Brawijaya1
Anisa Millah TaqiyyahUniversity of Brawijaya1
Mohammad FadjarUniversity of Brawijaya1
Riduwan PrasetyaState University of Malang1
Syafira Bilqis KhoyrohState University of Malang1

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OAI-PMH (metadata jurnal) http://teknomekanik.ppj.unp.ac.id/index.php/teknomekanik/oai, pertama di-harvest 10 Nov 2026, terakhir terlihat 16 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/  http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
	<dc:title xml:lang="en">Characteristics of sisal-epoxy composite boards with sodium chloride-treated fibers at different treatment temperatures</dc:title>
	<dc:creator xml:lang="en">Setyayunita, Tamaryska </dc:creator>
	<dc:creator xml:lang="en">Suryanto, Heru</dc:creator>
	<dc:creator xml:lang="en">Aminnudin, Aminnudin </dc:creator>
	<dc:creator xml:lang="en">Osman, Azlin Fazlina </dc:creator>
	<dc:creator xml:lang="en">Yanuhar, Uun</dc:creator>
	<dc:subject xml:lang="en">composite boards</dc:subject>
	<dc:subject xml:lang="en">mechanical properties</dc:subject>
	<dc:subject xml:lang="en">epoxy</dc:subject>
	<dc:subject xml:lang="en">NaCl treatment</dc:subject>
	<dc:subject xml:lang="en">sisal fiber</dc:subject>
	<dc:description xml:lang="en">The growing environmental concerns associated with synthetic fibers have led to the increased adoption of bio-fibers as reinforcements in polymer composites. Sodium chloride (NaCl) is explored as a fiber treatment agent to enhance the adhesion between fibers and the matrix. The study aims to evaluate the effects of NaCl treatment on the characteristics of sisal fiber-epoxy composite boards. A completely randomized design was applied with three factors: treatment temperature (25 °C and 100 °C), NaCl concentration (1, 3, and 5 wt%), and composite board density (0.40, 0.60, and 0.80 g/cm³). Sisal fibers were soaked in NaCl solutions for one hour, rinsed, dried, and manually blended with epoxy at a ratio of 80:20 wt%. Composite board properties were observed according to the standards of JIS-A-5908, Fourier Transform Infrared Spectroscopy (FTIR), and Scanning Electron Microscopy (SEM). Results indicated that increasing the NaCl concentration and treatment temperature significantly improved the properties of the composite board. The optimal parameters (5wt% NaCl, 100 °C, 0.80g/cm³) yielded a modulus of elasticity of 4.59±0.26 GPa, modulus of rupture of 18.88±0.03 MPa, and internal bond strength of 3.92±0.18 MPa, representing increases of 200.32%, 130.65%, and 218.70%, respectively. Thickness swelling decreased to 2.13±0.43% (48.14%) and water absorption to 8.95±0.05% (32.25%). These findings confirm that NaCl treatment is an eco-friendly method to enhance the mechanical strength and moisture resistance of biofiber composites. It also supports the development of high-performance composite boards.</dc:description>
	<dc:publisher xml:lang="en">Universitas Negeri Padang</dc:publisher>
	<dc:date>2025-06-30</dc:date>
	<dc:type>info:eu-repo/semantics/article</dc:type>
	<dc:type>info:eu-repo/semantics/publishedVersion</dc:type>
	<dc:format>application/pdf</dc:format>
	<dc:identifier>http://teknomekanik.ppj.unp.ac.id/index.php/teknomekanik/article/view/355</dc:identifier>
	<dc:identifier>10.24036/teknomekanik.v8i1.35572</dc:identifier>
	<dc:source xml:lang="en">Teknomekanik; Vol. 8 No. 1 (2025): Regular Issue; 38-51</dc:source>
	<dc:source>2621-8720</dc:source>
	<dc:source>2621-9980</dc:source>
	<dc:language>eng</dc:language>
	<dc:relation>http://teknomekanik.ppj.unp.ac.id/index.php/teknomekanik/article/view/355/93</dc:relation>
	<dc:rights xml:lang="en">Copyright (c) 2025 Tamaryska  Setyayunita, Heru Suryanto, Aminnudin  Aminnudin, Azlin Fazlina  Osman, Uun Yanuhar</dc:rights>
	<dc:rights xml:lang="en">http://creativecommons.org/licenses/by/4.0</dc:rights>
</oai_dc:dc>