The effect of FeNi-AlN layer thickness on the response of magnetic SAW sensor by FEM simulation
Bulletin of Electrical Engineering and Informatics · Vol. 13 No. 1 (2024) · hlm. 167–178
ISSN 2089-3191, 2302-9285
Terbit 2024-02-01
Penerbit Institute of Advanced Engineering and Science (IAES)
Bahasa en
Abstrak
In this study, we used simulation to investigate the optimal working point of a surface acoustic wave-magnetostriction sensor by varying the thickness of the magnetic sensitive layer using the finite elements method. We evaluated the sensor’s sensitivity by simulating the responses at the optimal point and changing the thickness of the magnetic sensitive layer (h3). Additionally, we reduced the piezoelectric substrate thickness (h1) at the optimal point to determine the limit point of the center frequency (f0) and improve the sensor sensitivity for low magnetic field intensity measurements by performing a wavelength reduction (λ). For the simulation, we selected a delay-line FeNi/IDT/AlN structure with specific materials and electrode parameters. Our results show that the optimal structure of the sensor is at h1=400 μm, λ=40 μm, and h3=1,060 nm, with a maximum f0 of 140.38493 MHz and maximum surface acoustic wave velocity of 5,615.4 m/s. At this optimal structure, the sensitivity reaches the maximum value of 10.287 kHz/Oe with a working range from 0 to 89 Oe. We also found that reducing the piezoelectric substrate thickness to 35 μm significantly reduces the manufacturing and simulation time, but the frequency response cannot determine the center frequency.
Jaringan kolaborasi para penulis
8 penulis ·
12 tautan kepenulisan bersama
· 2 lintas organisasi
Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.
Hanoi University of Science and Technology Phenikaa University Afiliasi tidak diketahui
Organisasi berbeda
Organisasi sama
Afiliasi tidak diketahui
Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.
Sumber metadata: OpenAlex API (jurnal SINTA, ADR 0048) https://openalex.org/S2765016208, pertama di-harvest 22 Nov 2026, terakhir terlihat 22 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/"><dc:title xml:lang="en">The effect of FeNi-AlN layer thickness on the response of magnetic SAW sensor by FEM simulation</dc:title><dc:creator>Do Duy Phu</dc:creator><dc:creator>Hoang Si Hong</dc:creator><dc:creator>Vinh V. Le</dc:creator><dc:subject>surface acoustic wave sensors</dc:subject><dc:subject>magnetostriction</dc:subject><dc:subject>layer thickness optimization</dc:subject><dc:subject>sensor sensitivity</dc:subject><dc:subject>IDT</dc:subject><dc:subject>center frequency</dc:subject><dc:subject>wavelength reduction</dc:subject><dc:subject>SAW velocity</dc:subject><dc:description xml:lang="en">In this study, we used simulation to investigate the optimal working point of a surface acoustic wave-magnetostriction sensor by varying the thickness of the magnetic sensitive layer using the finite elements method. We evaluated the sensor’s sensitivity by simulating the responses at the optimal point and changing the thickness of the magnetic sensitive layer (h3). Additionally, we reduced the piezoelectric substrate thickness (h1) at the optimal point to determine the limit point of the center frequency (f0) and improve the sensor sensitivity for low magnetic field intensity measurements by performing a wavelength reduction (λ). For the simulation, we selected a delay-line FeNi/IDT/AlN structure with specific materials and electrode parameters. Our results show that the optimal structure of the sensor is at h1=400 μm, λ=40 μm, and h3=1,060 nm, with a maximum f0 of 140.38493 MHz and maximum surface acoustic wave velocity of 5,615.4 m/s. At this optimal structure, the sensitivity reaches the maximum value of 10.287 kHz/Oe with a working range from 0 to 89 Oe. We also found that reducing the piezoelectric substrate thickness to 35 μm significantly reduces the manufacturing and simulation time, but the frequency response cannot determine the center frequency.</dc:description><dc:publisher>Institute of Advanced Engineering and Science (IAES)</dc:publisher><dc:date>2024-02-01</dc:date><dc:type>info:eu-repo/semantics/article</dc:type><dc:format>application/pdf</dc:format><dc:identifier>http://dx.doi.org/10.11591/eei.v13i1.6312</dc:identifier><dc:identifier>10.11591/eei.v13i1.6312</dc:identifier><dc:source>Bulletin of Electrical Engineering and Informatics; Vol 13 No 1 (2024); 167-178</dc:source><dc:source>2089-3191</dc:source><dc:source>2302-9285</dc:source><dc:language>en</dc:language><dc:relation>https://beei.org/index.php/EEI/article/download/6312/3528</dc:relation><dc:rights>https://creativecommons.org/licenses/by-sa/4.0/</dc:rights></oai_dc:dc>
Sitasi dan pengindeksan
OpenAlex
Terindeks
lewat ID karya OpenAlex (record dari sumber OpenAlex)
1 sitasi
Crossref
Terindeks
lewat DOI
0 sitasi
Jumlah menurut tiap indeks pada 19 Nov 2026; setiap indeks menghitung sitasi dengan cara berbeda.
OpenAlex juga mencatat karya ini di: crossref.
Sitasi artikel ini
APA 7
Phu, D. D., Hong, H. S., & Le, V. V. (2024). The effect of FeNi-AlN layer thickness on the response of magnetic SAW sensor by FEM simulation. Bulletin of Electrical Engineering and Informatics, 13(1), 167–178. https://doi.org/10.11591/eei.v13i1.6312
Salin
IEEE
D. D. Phu, H. S. Hong, and V. V. Le, “The effect of FeNi-AlN layer thickness on the response of magnetic SAW sensor by FEM simulation,” Bulletin of Electrical Engineering and Informatics, vol. 13, no. 1, pp. 167–178, 2024, doi: 10.11591/eei.v13i1.6312.
Salin
Dibuat dari metadata jurnal; periksa nama penulis sebelum dipakai.