Study of the Synthesis of Zirconia Powder from Zircon Sand obtained from Zircon Minerals Malaysia by Caustic Fusion Method

Indonesian Journal of Chemistry · Vol. 20 No. 4 (2020) · hlm. 782–782

DOI
10.22146/ijc.43936
ISSN
1411-9420, 2460-1578
Terbit
2020-06-10
Penerbit
Gadjah Mada University
Bahasa
en
Lisensi
creativecommons.org/licenses/by-nc-nd/4.0/

Abstrak

The zircon powder from Zircon Minerals Malaysia is a pure premium grade zircon sand milled 1.5 µm that contain ZrSiO4, ZrO2, HfO2, SiO2, Al2O3, TiO2, and Fe2O3. The monoclinic zirconia powders were synthesized from the zircon sand of Zircon Minerals Malaysia, by caustic fusion method at calcination temperatures between 500 °C to 800 °C. The as-synthesized zirconia was characterized through X-Ray diffraction (XRD), scanning electron microscopy (SEM), thermogravimetric and differential thermal analysis (TG-DTA), and X-Ray fluorescence (XRF) techniques. The XRD results show two monoclinic phases of microcrystalline zirconia. Zirconia that was calcined at 600 °C obtained the highest value of ZrO2, which was 54.48%; followed by zirconia calcined at 700 °C, 800 °C, and 500 °C, which obtained the ZrO2 values of 53.58%, 52.41%, and 51.53%, respectively, based on the XRF analysis. As-synthesized zirconia showed monoclinic phases where the surface areas were 0.0635 m2/g, 0.135 m2/g, 0.0268 m2/g, and 0.0288 m2/g, for zirconia calcined at temperatures of 500 °C, 600 °C, 700 °C, and 800 °C, respectively. The surface structure of the powder that had been calcined at 600 C showed similarities with the commercial zirconia. The similarities of the synthesized zirconia and commercial zirconia showed that the zirconia powder could be synthesized using zircon sand by caustic fusion method, even though the content of zirconia was lower compared to that of the commercial zirconia powder.

Kata kunci

Jaringan kolaborasi para penulis

4 penulis · 6 tautan kepenulisan bersama · 3 lintas organisasi

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • Universiti Teknologi MARA
  • Sirim Berhad
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OpenAlex API (jurnal SINTA, ADR 0048) https://openalex.org/S2764840418, pertama di-harvest 19 Nov 2026, terakhir terlihat 22 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/"><dc:title xml:lang="en">Study of the Synthesis of Zirconia Powder from Zircon Sand obtained from Zircon Minerals Malaysia by Caustic Fusion Method</dc:title><dc:creator>Istikamah Subuki</dc:creator><dc:creator>Mimi Fazzlinda Mohsin</dc:creator><dc:creator>Muhammad Hussain Ismail</dc:creator><dc:creator>Fazira Suriani Mohamed Fadzil</dc:creator><dc:subject>zirconia powder</dc:subject><dc:subject>zircon sand</dc:subject><dc:subject>calcination temperature</dc:subject><dc:subject>monoclinic zirconia</dc:subject><dc:subject>surface area</dc:subject><dc:subject>ZrO2 content</dc:subject><dc:description xml:lang="en">The zircon powder from Zircon Minerals Malaysia is a pure premium grade zircon sand milled 1.5 µm that contain ZrSiO4, ZrO2, HfO2, SiO2, Al2O3, TiO2, and Fe2O3. The monoclinic zirconia powders were synthesized from the zircon sand of Zircon Minerals Malaysia, by caustic fusion method at calcination temperatures between 500 °C to 800 °C. The as-synthesized zirconia was characterized through X-Ray diffraction (XRD), scanning electron microscopy (SEM), thermogravimetric and differential thermal analysis (TG-DTA), and X-Ray fluorescence (XRF) techniques. The XRD results show two monoclinic phases of microcrystalline zirconia. Zirconia that was calcined at 600 °C obtained the highest value of ZrO2, which was 54.48%; followed by zirconia calcined at 700 °C, 800 °C, and 500 °C, which obtained the ZrO2 values of 53.58%, 52.41%, and 51.53%, respectively, based on the XRF analysis. As-synthesized zirconia showed monoclinic phases where the surface areas were 0.0635 m2/g, 0.135 m2/g, 0.0268 m2/g, and 0.0288 m2/g, for zirconia calcined at temperatures of 500 °C, 600 °C, 700 °C, and 800 °C, respectively. The surface structure of the powder that had been calcined at 600 C showed similarities with the commercial zirconia. The similarities of the synthesized zirconia and commercial zirconia showed that the zirconia powder could be synthesized using zircon sand by caustic fusion method, even though the content of zirconia was lower compared to that of the commercial zirconia powder.</dc:description><dc:publisher>Gadjah Mada University</dc:publisher><dc:date>2020-06-10</dc:date><dc:type>info:eu-repo/semantics/article</dc:type><dc:format>application/pdf</dc:format><dc:identifier>https://doi.org/10.22146/ijc.43936</dc:identifier><dc:identifier>10.22146/ijc.43936</dc:identifier><dc:source>Indonesian Journal of Chemistry; Vol 20 No 4 (2020); 782-782</dc:source><dc:source>1411-9420</dc:source><dc:source>2460-1578</dc:source><dc:language>en</dc:language><dc:relation>https://jurnal.ugm.ac.id/ijc/article/download/43936/25853</dc:relation><dc:rights>https://creativecommons.org/licenses/by-nc-nd/4.0/</dc:rights></oai_dc:dc>