Synthesis of Mesoporous Carbon from Merbau Wood (Intsia spp.) by Microwave Method as Ni Catalyst Support for α-Cellulose Hydrocracking

Indonesian Journal of Chemistry (2019)

DOI
10.22146/ijc.34189
ISSN
1411-9420, 2460-1578
Terbit
2019-04-11
Penerbit
Gadjah Mada University
Bahasa
en
Lisensi
creativecommons.org/licenses/by-nc-nd/4.0/

Abstrak

Synthesis of mesoporous carbon from Merbau wood (Intsia spp.) waste by microwave method as nickel catalyst support for α-cellulose hydrocracking had been carried out. The Merbau wood sawdust was carbonized at 800 °C to produce C800 and the C800 was treated by microwave irradiation (399 W) for 5 min to produce C800MW. The Merbau wood flakes, which were only treated by microwave irradiation (399 Watts) for 30 min produced CMW. Wet impregnation technique was carried out to disperse the Ni metal (1.0, 1.5, and 2.0 wt.%) onto the best mesoporous carbon. The mesoporous carbons were analyzed by Fourier Transform Infra-Red Spectroscopy (FTIR), Surface Area Analyzer (SAA) and Scanning Electron Microscopy (SEM). The hydrocracking of pyrolyzed α-cellulose was carried out at 400 °C. The liquid product was analyzed by Gas Chromatograph-Mass Spectrometer (GC-MS). The results showed that the C800MW was the best performance carbon and it had a specific surface area, total pore volume, average pore diameter and acidity of 364.12 m2/g, 0.28 cm3/g, 3.03 nm, and 2.18 mmol/g, respectively. The Ni1.5/C800MW catalyst produced the highest conversion of liquid product (58.76 wt.%) than the Ni1/C800MW (57.51 wt.%) and Ni2/C800MW (34.18 wt.%).

Kata kunci

Jaringan kolaborasi para penulis

40 penulis · 156 tautan kepenulisan bersama · 32 lintas organisasi · menampilkan 40 yang paling banyak terhubung

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • Universitas Gadjah Mada
  • Institut Teknologi Sepuluh Nopember
  • Pertamina (Indonesia)
  • Sebelas Maret University
  • Leipzig University
  • State University of Semarang
  • Universitas Ahmad Dahlan
  • Afiliasi tidak diketahui
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama
Dyah Ayu FatmawatiUniversitas Gadjah Mada23
Uswatul ChasanahUniversitas Gadjah Mada9
Suryo PurwonoUniversitas Gadjah Mada8
Haryo Satriya OktavianoPertamina (Indonesia)6
Cahyarani ParamestiUniversitas Gadjah Mada6
Savitri LarasatiUniversitas Gadjah Mada6
Nugroho Raka SantosoUniversitas Gadjah Mada6
Endang Tri WahyuniUniversitas Gadjah Mada5
Sri Juari SantosaUniversitas Gadjah Mada5
Akhmad SyoufianUniversitas Gadjah Mada5
Sri SudionoUniversitas Gadjah Mada5
Maria UlfaSebelas Maret University5
Indriana KartiniUniversitas Gadjah Mada5
Satriyo Dibyo SumbogoUniversitas Gadjah Mada5
Harno Dwi PranowoUniversitas Gadjah Mada4
TriyonoAfiliasi tidak diketahui4
Sutarno SutarnoUniversitas Gadjah Mada4
Karna WijayaUniversitas Gadjah Mada4
Mokhammad Fajar PradiptaUniversitas Gadjah Mada4
Endah SuarsihUniversitas Gadjah Mada4
Hendro JuwonoInstitut Teknologi Sepuluh Nopember3
Dwi SiswantaUniversitas Gadjah Mada3
Rian KurniawanLeipzig University3
Puspa Nindro MahayuwatiUniversitas Gadjah Mada3
Mudasir MudasirUniversitas Gadjah Mada3
Didik PrasetyokoInstitut Teknologi Sepuluh Nopember3
Bambang SetiajiUniversitas Gadjah Mada3
Iqmal TahirUniversitas Gadjah Mada3
Edy CahyonoState University of Semarang2
Siti SalamahUniversitas Ahmad Dahlan2
Iman SantosoUniversitas Gadjah Mada2
Ita UlfinInstitut Teknologi Sepuluh Nopember2
M. MuchalalUniversitas Gadjah Mada2
Karna WijayaUniversitas Gadjah Mada2

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OpenAlex API (jurnal SINTA, ADR 0048) https://openalex.org/S2764840418, pertama di-harvest 19 Nov 2026, terakhir terlihat 19 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/"><dc:title xml:lang="en">Synthesis of Mesoporous Carbon from Merbau Wood (Intsia spp.) by Microwave Method as Ni Catalyst Support for α-Cellulose Hydrocracking</dc:title><dc:creator>Andaru Dena Prasiwi</dc:creator><dc:creator>Wega Trisunaryanti</dc:creator><dc:creator>Triyono Triyono</dc:creator><dc:creator>Iip Izul Falah</dc:creator><dc:creator>Darma Santi</dc:creator><dc:creator>Muhammad Fajar Marsuki</dc:creator><dc:subject>mesoporous carbon</dc:subject><dc:subject>microwave-assisted carbonization</dc:subject><dc:subject>sawdust</dc:subject><dc:subject>biomass-derived carbon</dc:subject><dc:subject>wet impregnation</dc:subject><dc:subject>catalyst acidity</dc:subject><dc:subject>liquid yield</dc:subject><dc:description xml:lang="en">Synthesis of mesoporous carbon from Merbau wood (Intsia spp.) waste by microwave method as nickel catalyst support for α-cellulose hydrocracking had been carried out. The Merbau wood sawdust was carbonized at 800 °C to produce C800 and the C800 was treated by microwave irradiation (399 W) for 5 min to produce C800MW. The Merbau wood flakes, which were only treated by microwave irradiation (399 Watts) for 30 min produced CMW. Wet impregnation technique was carried out to disperse the Ni metal (1.0, 1.5, and 2.0 wt.%) onto the best mesoporous carbon. The mesoporous carbons were analyzed by Fourier Transform Infra-Red Spectroscopy (FTIR), Surface Area Analyzer (SAA) and Scanning Electron Microscopy (SEM). The hydrocracking of pyrolyzed α-cellulose was carried out at 400 °C. The liquid product was analyzed by Gas Chromatograph-Mass Spectrometer (GC-MS). The results showed that the C800MW was the best performance carbon and it had a specific surface area, total pore volume, average pore diameter and acidity of 364.12 m2/g, 0.28 cm3/g, 3.03 nm, and 2.18 mmol/g, respectively. The Ni1.5/C800MW catalyst produced the highest conversion of liquid product (58.76 wt.%) than the Ni1/C800MW (57.51 wt.%) and Ni2/C800MW (34.18 wt.%).</dc:description><dc:publisher>Gadjah Mada University</dc:publisher><dc:date>2019-04-11</dc:date><dc:type>info:eu-repo/semantics/article</dc:type><dc:identifier>https://doi.org/10.22146/ijc.34189</dc:identifier><dc:identifier>10.22146/ijc.34189</dc:identifier><dc:source>Indonesian Journal of Chemistry; (2019)</dc:source><dc:source>1411-9420</dc:source><dc:source>2460-1578</dc:source><dc:language>en</dc:language><dc:rights>https://creativecommons.org/licenses/by-nc-nd/4.0/</dc:rights></oai_dc:dc>