Synthesis of Low TENORM Zirconium Sulfate from ZrO(OH)2 with Sulfuric Acid

Indonesian Journal of Chemistry · Vol. 21 No. 4 (2021) · hlm. 842–842

DOI
10.22146/ijc.60298
ISSN
1411-9420, 2460-1578
Terbit
2021-05-21
Penerbit
Gadjah Mada University
Bahasa
en
Lisensi
creativecommons.org/licenses/by-nc-nd/4.0/

Abstrak

Zirconium sulfate (ZS) has become one of the alternative chemical compounds for substituting traditional tannery substances using chromium(III) which was not environmentally friendly. The purpose of this research was to synthesize ZS from ZrO(OH)2 using H2SO4 with low Technologically Naturally Occurring Radioactive Material (TENORM) content. This ZS synthesis process shortened the old processing flow at which plenty of chemical reactors were used. The results showed that with 300 mg of feed, 600 mL of 95% H2SO4, at a temperature of 250 °C, the contact time of 150 min, the obtained conversion was 77.76%. Furthermore, in this 95% acid leaching reactor, the SiO2 content was still 2.79% and it was not TENORM free yet, but the FTIR and XRD images were in accordance with BDH standards. Moreover, the quenching process results had been free of SiO2 and TENORM content, but they still contained 1.48% HfO2. The surface of the TEM images from the quenching results had been in the form of elongated and transparent crystals. The result of the economic feasibility analysis showed that the new ZS synthesis process was more economical or profitable when it was compared to the old ZS synthesis process, with a BCR value of 1.258.

Kata kunci

Jaringan kolaborasi para penulis

5 penulis · 4 tautan kepenulisan bersama

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • National Nuclear Energy Agency of Indonesia
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama
C. SupriyantoNational Nuclear Energy Agency of Indonesia1
Maria Veronica PurwaniNational Nuclear Energy Agency of Indonesia1
Herry PoernomoNational Nuclear Energy Agency of Indonesia1

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OpenAlex API (jurnal SINTA, ADR 0048) https://openalex.org/S2764840418, pertama di-harvest 19 Nov 2026, terakhir terlihat 19 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/"><dc:title xml:lang="en">Synthesis of Low TENORM Zirconium Sulfate from ZrO(OH)2 with Sulfuric Acid</dc:title><dc:creator>Rahmatika Alfia Amiliana</dc:creator><dc:creator>Muzakky Muzakky</dc:creator><dc:subject>zirconium sulfate</dc:subject><dc:subject>zirconium oxyhydroxide</dc:subject><dc:subject>sulfuric acid leaching</dc:subject><dc:subject>TENORM</dc:subject><dc:subject>quenching</dc:subject><dc:subject>silicon dioxide removal</dc:subject><dc:subject>hafnium oxide</dc:subject><dc:subject>economic feasibility</dc:subject><dc:description xml:lang="en">Zirconium sulfate (ZS) has become one of the alternative chemical compounds for substituting traditional tannery substances using chromium(III) which was not environmentally friendly. The purpose of this research was to synthesize ZS from ZrO(OH)2 using H2SO4 with low Technologically Naturally Occurring Radioactive Material (TENORM) content. This ZS synthesis process shortened the old processing flow at which plenty of chemical reactors were used. The results showed that with 300 mg of feed, 600 mL of 95% H2SO4, at a temperature of 250 °C, the contact time of 150 min, the obtained conversion was 77.76%. Furthermore, in this 95% acid leaching reactor, the SiO2 content was still 2.79% and it was not TENORM free yet, but the FTIR and XRD images were in accordance with BDH standards. Moreover, the quenching process results had been free of SiO2 and TENORM content, but they still contained 1.48% HfO2. The surface of the TEM images from the quenching results had been in the form of elongated and transparent crystals. The result of the economic feasibility analysis showed that the new ZS synthesis process was more economical or profitable when it was compared to the old ZS synthesis process, with a BCR value of 1.258.</dc:description><dc:publisher>Gadjah Mada University</dc:publisher><dc:date>2021-05-21</dc:date><dc:type>info:eu-repo/semantics/article</dc:type><dc:format>application/pdf</dc:format><dc:identifier>https://doi.org/10.22146/ijc.60298</dc:identifier><dc:identifier>10.22146/ijc.60298</dc:identifier><dc:source>Indonesian Journal of Chemistry; Vol 21 No 4 (2021); 842-842</dc:source><dc:source>1411-9420</dc:source><dc:source>2460-1578</dc:source><dc:language>en</dc:language><dc:relation>https://jurnal.ugm.ac.id/ijc/article/download/60298/31036</dc:relation><dc:rights>https://creativecommons.org/licenses/by-nc-nd/4.0/</dc:rights></oai_dc:dc>