Microstructure Analysis of Synthesized LiBOB
Indonesian Journal of Chemistry · Vol. 15 No. 3 (2015) · hlm. 242–247
ISSN 1411-9420, 2460-1578
Terbit 2015-11-12
Penerbit Gadjah Mada University
Bahasa en
Abstrak
Lithium bis (oxalate) borate or LiBOB is an active material used as the electrolyte for lithium battery application. LiBOB (LiB(C2O4)2) powder was prepared from LiOH, H2C2O4 and H3BO3. The employed method was solid state reaction. LiBOB powder produced from the reaction was then observed using SEM and TEM. Surface area was analyzed using Quantachrome Nova 4200e. From the analysis analyzed using XRD to identify the resulting phases, crystal structure, and crystallite size. The functional groups were analyzed using FT-IR. The particle morphology was result, it was seen that the resulted phases were C4LiBO8 and LiB(C2O4)2.H2O, the crystal structure was orthorhombic with space group Pbca and Pnma. From the particle morphology observation it was shown that micro pores were created irregularly. When the observation was deepened, nanopores with elongated round shape were seen within the micropores. The pore size was approximately 50–100 nm. The surface area, total pore volume, and average pore diameter of LiBOB powder was 88.556 m2/g, 0.4252 cm3/g, and 19.2 nm respectively.
Jaringan kolaborasi para penulis
16 penulis ·
39 tautan kepenulisan bersama
· 17 lintas organisasi
Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.
Indonesian Institute of Sciences University of Indonesia Diponegoro University IPB University
Organisasi berbeda
Organisasi sama
Afiliasi tidak diketahui
Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.
Sumber metadata: OpenAlex API (jurnal SINTA, ADR 0048) https://openalex.org/S2764840418, pertama di-harvest 19 Nov 2026, terakhir terlihat 19 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/"><dc:title xml:lang="en">Microstructure Analysis of Synthesized LiBOB</dc:title><dc:creator>Etty Marti Wigayati</dc:creator><dc:creator>Christin Rina Ratri</dc:creator><dc:creator>Ibrahim Purawiardi</dc:creator><dc:creator>Fadli Rohman</dc:creator><dc:creator>Titik Lestariningsih</dc:creator><dc:subject>lithium bis(oxalate)borate</dc:subject><dc:subject>LiBOB</dc:subject><dc:subject>lithium battery electrolytes</dc:subject><dc:subject>solid-state synthesis</dc:subject><dc:subject>crystal structure</dc:subject><dc:subject>orthorhombic phase</dc:subject><dc:subject>particle morphology</dc:subject><dc:subject>nanopores</dc:subject><dc:subject>pore size distribution</dc:subject><dc:subject>specific surface area</dc:subject><dc:description xml:lang="en">Lithium bis (oxalate) borate or LiBOB is an active material used as the electrolyte for lithium battery application. LiBOB (LiB(C2O4)2) powder was prepared from LiOH, H2C2O4 and H3BO3. The employed method was solid state reaction. LiBOB powder produced from the reaction was then observed using SEM and TEM. Surface area was analyzed using Quantachrome Nova 4200e. From the analysis analyzed using XRD to identify the resulting phases, crystal structure, and crystallite size. The functional groups were analyzed using FT-IR. The particle morphology was result, it was seen that the resulted phases were C4LiBO8 and LiB(C2O4)2.H2O, the crystal structure was orthorhombic with space group Pbca and Pnma. From the particle morphology observation it was shown that micro pores were created irregularly. When the observation was deepened, nanopores with elongated round shape were seen within the micropores. The pore size was approximately 50–100 nm. The surface area, total pore volume, and average pore diameter of LiBOB powder was 88.556 m2/g, 0.4252 cm3/g, and 19.2 nm respectively.</dc:description><dc:publisher>Gadjah Mada University</dc:publisher><dc:date>2015-11-12</dc:date><dc:type>info:eu-repo/semantics/article</dc:type><dc:identifier>https://doi.org/10.22146/ijc.21191</dc:identifier><dc:identifier>10.22146/ijc.21191</dc:identifier><dc:source>Indonesian Journal of Chemistry; Vol 15 No 3 (2015); 242-247</dc:source><dc:source>1411-9420</dc:source><dc:source>2460-1578</dc:source><dc:language>en</dc:language><dc:rights>https://creativecommons.org/licenses/by-nc-nd/4.0/</dc:rights></oai_dc:dc>
Sitasi dan pengindeksan
OpenAlex
Terindeks
lewat ID karya OpenAlex (record dari sumber OpenAlex)
10 sitasi
Crossref
Belum diperiksa
Jumlah menurut tiap indeks pada 19 Nov 2026; setiap indeks menghitung sitasi dengan cara berbeda.
OpenAlex juga mencatat karya ini di: crossref, doaj.
Sitasi artikel ini
APA 7
Wigayati, E. M., Ratri, C. R., Purawiardi, I., Rohman, F., & Lestariningsih, T. (2015). Microstructure Analysis of Synthesized LiBOB. Indonesian Journal of Chemistry, 15(3), 242–247. https://doi.org/10.22146/ijc.21191
Salin
IEEE
E. M. Wigayati, C. R. Ratri, I. Purawiardi, F. Rohman, and T. Lestariningsih, “Microstructure Analysis of Synthesized LiBOB,” Indonesian Journal of Chemistry, vol. 15, no. 3, pp. 242–247, 2015, doi: 10.22146/ijc.21191.
Salin
Dibuat dari metadata jurnal; periksa nama penulis sebelum dipakai.