Morphology of NdFeB-Type Permanent Magnet Coercivity Enhancement by Heat Treatment Process

Indonesian Journal of Chemistry · Vol. 21 No. 3 (2020) · hlm. 626–626

DOI
10.22146/ijc.59096
ISSN
1411-9420, 2460-1578
Terbit
2020-12-22
Penerbit
Gadjah Mada University
Bahasa
en
Lisensi
creativecommons.org/licenses/by-nc-nd/4.0/

Abstrak

To understand the morphology of the coercivity enhancement by heat treatment, a commercial sintered NdFeB-type permanent magnet is annealed, and the coercivity is measured by Permagraph. It is shown that the coercivity is increased compared to the initial. Observation by X-Ray Diffraction (XRD) analysis and Scanning Electron Microscope-Energy Dispersive X-ray Spectroscopy (SEM-EDS) is then conducted. The XRD result shows the amount of NdFeB content in the NdFeB-type permanent magnet is increased after heat treatment. The more significant amount of NdFeB content causes higher coercivity. The maximum coercivity, 19 kOe, is achieved at 850 °C of heat treatment temperature, where the NdFeB content is at the highest amount. Microstructural characterizations using SEM-EDS show that at 850 °C of heat treatment temperature, the iron (Fe) content in the grain boundaries is the lowest. It causes higher coercivity. This is due to the magnetically decoupled between NdFeB grains. The decoupling magnet of the NdFeB grains is affected by the Fe content in the grain boundaries. High-temperature heat treatment at 900 and 1050 °C led to the decomposition of NdFeB content in the grains and increased the Fe content in the grain boundaries, which resulted in a substantial reduction of magnetic coercivity.

Kata kunci

Jaringan kolaborasi para penulis

6 penulis · 15 tautan kepenulisan bersama · 5 lintas organisasi

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • Ministry of Industry of the Republic of Indonesia
  • Universitas Jenderal Achmad Yani
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OpenAlex API (jurnal SINTA, ADR 0048) https://openalex.org/S2764840418, pertama di-harvest 19 Nov 2026, terakhir terlihat 22 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/"><dc:title xml:lang="en">Morphology of NdFeB-Type Permanent Magnet Coercivity Enhancement by Heat Treatment Process</dc:title><dc:creator>Eva Afrilinda</dc:creator><dc:creator>Dagus Resmana Djuanda</dc:creator><dc:creator>Shinta Virdhian</dc:creator><dc:creator>Martin Doloksaribu</dc:creator><dc:creator>Moch Iqbal Zaelana Muttahar</dc:creator><dc:creator>Sri Bimo Pratomo</dc:creator><dc:subject>Nd-Fe-B permanent magnets</dc:subject><dc:subject>coercivity enhancement</dc:subject><dc:subject>heat treatment</dc:subject><dc:subject>sintered magnets</dc:subject><dc:subject>annealing</dc:subject><dc:subject>microstructure</dc:subject><dc:description xml:lang="en">To understand the morphology of the coercivity enhancement by heat treatment, a commercial sintered NdFeB-type permanent magnet is annealed, and the coercivity is measured by Permagraph. It is shown that the coercivity is increased compared to the initial. Observation by X-Ray Diffraction (XRD) analysis and Scanning Electron Microscope-Energy Dispersive X-ray Spectroscopy (SEM-EDS) is then conducted. The XRD result shows the amount of NdFeB content in the NdFeB-type permanent magnet is increased after heat treatment. The more significant amount of NdFeB content causes higher coercivity. The maximum coercivity, 19 kOe, is achieved at 850 °C of heat treatment temperature, where the NdFeB content is at the highest amount. Microstructural characterizations using SEM-EDS show that at 850 °C of heat treatment temperature, the iron (Fe) content in the grain boundaries is the lowest. It causes higher coercivity. This is due to the magnetically decoupled between NdFeB grains. The decoupling magnet of the NdFeB grains is affected by the Fe content in the grain boundaries. High-temperature heat treatment at 900 and 1050 °C led to the decomposition of NdFeB content in the grains and increased the Fe content in the grain boundaries, which resulted in a substantial reduction of magnetic coercivity.</dc:description><dc:publisher>Gadjah Mada University</dc:publisher><dc:date>2020-12-22</dc:date><dc:type>info:eu-repo/semantics/article</dc:type><dc:format>application/pdf</dc:format><dc:identifier>https://doi.org/10.22146/ijc.59096</dc:identifier><dc:identifier>10.22146/ijc.59096</dc:identifier><dc:source>Indonesian Journal of Chemistry; Vol 21 No 3 (2020); 626-626</dc:source><dc:source>1411-9420</dc:source><dc:source>2460-1578</dc:source><dc:language>en</dc:language><dc:relation>https://jurnal.ugm.ac.id/ijc/article/download/59096/29932</dc:relation><dc:rights>https://creativecommons.org/licenses/by-nc-nd/4.0/</dc:rights></oai_dc:dc>