THE USE OF FLY ASH AND ZEOLITE MIXTURE AS BACKFILL MATERIAL IN THE RADIOACTIVE WASTE REPOSITORY

Indonesian Journal of Chemistry · Vol. 5 No. 3 (2010) · hlm. 302–308

DOI
10.22146/ijc.21808
ISSN
1411-9420, 2460-1578
Terbit
2010-06-15
Penerbit
Gadjah Mada University
Bahasa
en
Lisensi
creativecommons.org/licenses/by-nc-nd/4.0/

Abstrak

An investigation of the contribution of fly ash in the fly ash-zeolite mixture as the backfill material on the shallow land burial of radioactive waste has been done. The experiment objective is to know the effect of zeolite particle size and fly ash-zeolite weight ratio on physical properties such as permeability (K) and dispersion characteristic such as effective dispersion coefficient (De) in the fly ash-zeolite form as backfill material. The experiment was carried out by the fixed bed method in the column filled by the fly ash-zeolite mixture with a fly ash-to-zeolite weight percent ratio of 100/0, 80/20, 60/40, 40/60, 20/80, 0/100 in the water saturated condition flown by uranyl nitrate solution at concentration (Co) of 500 ppm. The concentration of uranium in the effluents in interval 15 minutes represented as Ct was analyzed by spectrophotometer, then using Co and Ct, data effective dispersion coefficient (De) in the backfill material were determined. The experiment data showed that -400 mesh fly ash and -70+80 mesh zeolite on fly ash-to-zeolite with weight percent ratio of 40/60 with K = 5.00x10-5cm/second and De = 1.11.10-5 cm2/second can be used as backfill material. Keywords: backfill material, fly ash, radioactive waste, zeolite

Kata kunci

Jaringan kolaborasi para penulis

5 penulis · 5 tautan kepenulisan bersama

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • National Nuclear Energy Agency of Indonesia
  • Afiliasi tidak diketahui
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama
Cahya WidiyatiAfiliasi tidak diketahui1
Muzakky MuzakkyNational Nuclear Energy Agency of Indonesia1

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OpenAlex API (jurnal SINTA, ADR 0048) https://openalex.org/S2764840418, pertama di-harvest 19 Nov 2026, terakhir terlihat 19 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/"><dc:title xml:lang="en">THE USE OF FLY ASH AND ZEOLITE MIXTURE AS BACKFILL MATERIAL IN THE RADIOACTIVE WASTE REPOSITORY</dc:title><dc:creator>Herry Poernomo</dc:creator><dc:creator>Noor Anis Kundari</dc:creator><dc:creator>J W Burhani</dc:creator><dc:subject>fly ash</dc:subject><dc:subject>zeolites</dc:subject><dc:subject>backfill material</dc:subject><dc:subject>nuclear waste repository</dc:subject><dc:subject>shallow land burial</dc:subject><dc:subject>permeability</dc:subject><dc:subject>effective dispersion coefficient</dc:subject><dc:subject>uranium transport</dc:subject><dc:subject>uranyl nitrate</dc:subject><dc:subject>particle size</dc:subject><dc:description xml:lang="en">An investigation of the contribution of fly ash in the fly ash-zeolite mixture as the backfill material on the shallow land burial of radioactive waste has been done. The experiment objective is to know the effect of zeolite particle size and fly ash-zeolite weight ratio on physical properties such as permeability (K) and dispersion characteristic such as effective dispersion coefficient (De) in the fly ash-zeolite form as backfill material. The experiment was carried out by the fixed bed method in the column filled by the fly ash-zeolite mixture with a fly ash-to-zeolite weight percent ratio of 100/0, 80/20, 60/40, 40/60, 20/80, 0/100 in the water saturated condition flown by uranyl nitrate solution at concentration (Co) of 500 ppm. The concentration of uranium in the effluents in interval 15 minutes represented as Ct was analyzed by spectrophotometer, then using Co and Ct, data effective dispersion coefficient (De) in the backfill material were determined. The experiment data showed that -400 mesh fly ash and -70+80 mesh zeolite on fly ash-to-zeolite with weight percent ratio of 40/60 with K = 5.00x10-5cm/second and De = 1.11.10-5 cm2/second can be used as backfill material. Keywords: backfill material, fly ash, radioactive waste, zeolite</dc:description><dc:publisher>Gadjah Mada University</dc:publisher><dc:date>2010-06-15</dc:date><dc:type>info:eu-repo/semantics/article</dc:type><dc:identifier>https://doi.org/10.22146/ijc.21808</dc:identifier><dc:identifier>10.22146/ijc.21808</dc:identifier><dc:source>Indonesian Journal of Chemistry; Vol 5 No 3 (2010); 302-308</dc:source><dc:source>1411-9420</dc:source><dc:source>2460-1578</dc:source><dc:language>en</dc:language><dc:rights>https://creativecommons.org/licenses/by-nc-nd/4.0/</dc:rights></oai_dc:dc>