Melola Discovery

← Melola Discovery

Akses terbuka Jurnal SINTA 1

Preparation and Performance Evaluation of Magnetic Heterostructure Fe3O4@TiO2 Nanocomposite-Based Photocatalyst for Degradation of Methylene Blue Dye Under Direct Sunlight Irradiation

Indonesian Journal of Chemistry · Vol. 26 No. 6 (2026) · hlm. 1803–1803

DOI
10.22146/ijc.110581
ISSN
1411-9420, 2460-1578
Terbit
2026-11-03
Penerbit
Gadjah Mada University
Bahasa
en
Lisensi
creativecommons.org/licenses/by-nc-nd/4.0/

Abstrak

A magnetic Fe3O4@TiO2 nanocomposite photocatalyst was prepared and applied for the photocatalytic degradation of methylene blue under UV-vis light and direct sunlight. The prepared photocatalyst was characterized using XRD, FE-SEM, HR-TEM, and VSM. From morphological observations, the particles in the nanocomposite are tightly aggregated into spherical shapes, with lattice interlayer spacings of 0.24 and 0.33 nm, corresponding to the (311) plane of Fe3O4 and the (101) plane of anatase TiO2, respectively. The bandgap energy for the pure TiO2 is 3.2 eV, whereas it is 2.6 eV for the Fe3O4@TiO2, indicating that the introduction of Fe3O4 expands the photocatalytic activity in the visible region. The maximum photocatalytic efficiency recorded after 180 min under direct sunlight (58.00%) was lower than that under UV light (75.74%). These results are promising for practical applications, highlighting sunlight as a clean, viable, economical, and simple process option for removing organic dye pollutants from wastewater under ambient temperature and pressure. This study clearly shows that the sunlight-driven Fe3O4@TiO2 ambient-scale performance is lower than that at the laboratory scale under UV. Therefore, to achieve high photocatalytic degradation efficiency under direct sunlight, it is necessary to optimize the reactor design and also to dope Fe3O4@TiO2 into a complex system.

Kata kunci

Jaringan kolaborasi para penulis

6 penulis · 11 tautan kepenulisan bersama · 3 lintas organisasi

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • Université Nangui Abrogoua
  • Kenyatta University
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama
Kicoun Jean-Yves N’Zi ToureKenyatta University2
Kanga Marius N’GattaUniversité Nangui Abrogoua2

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OpenAlex API (jurnal SINTA, ADR 0048) https://openalex.org/S2764840418, pertama di-harvest 19 Nov 2026, terakhir terlihat 22 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/"><dc:title xml:lang="en">Preparation and Performance Evaluation of Magnetic Heterostructure Fe3O4@TiO2 Nanocomposite-Based Photocatalyst for Degradation of Methylene Blue Dye Under Direct Sunlight Irradiation</dc:title><dc:creator>Edja Florentin Assanvo</dc:creator><dc:creator>Ignace Christian M’Bra</dc:creator><dc:creator>Kouakou Vianet Bonsombra</dc:creator><dc:creator>David Boa</dc:creator><dc:subject>Fe3O4/TiO2 nanocomposite</dc:subject><dc:subject>magnetic photocatalyst</dc:subject><dc:subject>heterostructures</dc:subject><dc:subject>photocatalytic degradation</dc:subject><dc:subject>methylene blue</dc:subject><dc:subject>dye wastewater treatment</dc:subject><dc:subject>band gap narrowing</dc:subject><dc:subject>visible light photocatalysis</dc:subject><dc:subject>UV-Vis light</dc:subject><dc:subject>reactor design</dc:subject><dc:description xml:lang="en">A magnetic Fe3O4@TiO2 nanocomposite photocatalyst was prepared and applied for the photocatalytic degradation of methylene blue under UV-vis light and direct sunlight. The prepared photocatalyst was characterized using XRD, FE-SEM, HR-TEM, and VSM. From morphological observations, the particles in the nanocomposite are tightly aggregated into spherical shapes, with lattice interlayer spacings of 0.24 and 0.33 nm, corresponding to the (311) plane of Fe3O4 and the (101) plane of anatase TiO2, respectively. The bandgap energy for the pure TiO2 is 3.2 eV, whereas it is 2.6 eV for the Fe3O4@TiO2, indicating that the introduction of Fe3O4 expands the photocatalytic activity in the visible region. The maximum photocatalytic efficiency recorded after 180 min under direct sunlight (58.00%) was lower than that under UV light (75.74%). These results are promising for practical applications, highlighting sunlight as a clean, viable, economical, and simple process option for removing organic dye pollutants from wastewater under ambient temperature and pressure. This study clearly shows that the sunlight-driven Fe3O4@TiO2 ambient-scale performance is lower than that at the laboratory scale under UV. Therefore, to achieve high photocatalytic degradation efficiency under direct sunlight, it is necessary to optimize the reactor design and also to dope Fe3O4@TiO2 into a complex system.</dc:description><dc:publisher>Gadjah Mada University</dc:publisher><dc:date>2026-11-03</dc:date><dc:type>info:eu-repo/semantics/article</dc:type><dc:identifier>https://doi.org/10.22146/ijc.110581</dc:identifier><dc:identifier>10.22146/ijc.110581</dc:identifier><dc:source>Indonesian Journal of Chemistry; Vol 26 No 6 (2026); 1803-1803</dc:source><dc:source>1411-9420</dc:source><dc:source>2460-1578</dc:source><dc:language>en</dc:language><dc:rights>https://creativecommons.org/licenses/by-nc-nd/4.0/</dc:rights></oai_dc:dc>