Analisis Pengaruh Aliran Fluida Pendingin dan Waktu Pengelasan Spot Welding Kw14-1031 Terhadap Kekuatan Tarik Pelat Baja ST 40

Analisis Pengaruh Aliran Fluida Pendingin Dan Waktu Pengelasan Spot Welding Kw14-1031 Terhadap Kekuatan Tarik Pelat Baja ST 40

Journal of Applied Mechanical Engineering and Green Technology · Vol. 4 No. 1 (2026) · hlm. 8–13

DOI
10.31940/jametech.v4i1.8-13
ISSN
2684-8201, 2655-9145
Terbit
2026-04-24
Penerbit
Unit Publikasi Ilmiah, P3M, Politeknik Negeri Bali
Bahasa
ind

Abstrak

Inggris

Spot welding is greatly influenced by the cooling medium in terms of welding characteristics such as strength. The tensile strength of ST 40 steel plate welded joints is influenced by the cooling medium and welding time. Testing and data collection use experimental methods on spot welding machines and shear tests. Data collection uses quantitative methods while processing uses descriptive methods. The ASTM E8 standard is used in sample testing. The flow of coolant fluid in the spotwelding process significantly affects the HAZ diameter. Faster fluid flow increases heat transfer from the electrode to the coolant, keeping the electrode and weld material temperatures below 1,500 ºC, thereby reducing electrode wear and maintaining a stable weld nugget size at 5.00 mm. The lowest HAZ diameter was recorded at a flow rate of 5 liters/minute with a HAZ diameter of 8.30 mm, while the highest was at a flow rate of 2 liters/minute with a diameter of 10.43 mm. Too fast cooling or too short welding time can cause brittle weld joints and reduce tensile stress. Conversely, slower cooling with appropriate welding time produces optimal tensile strength while maintaining the structural integrity of the joint. Optimal results were found at a fluid flow rate of 2 liters/minute at 5.0 seconds with a tensile stress of 96.10 MPa, 3 liters/minute at 6.0 seconds with a tensile stress of 104.89 MPa, 4 liters/minute at 7.0 seconds with a tensile stress of 114.00 MPa and 5 liters/minute at 8.0 and 9.0 seconds with tensile stress of 116.72 MPa and 125.76 MPa.

Bahasa Indonesia

Media pendingin pada pengelasan ini sangat mempengaruhi karakteristik hasil pengelasan seperti kekuatan. Penempatan sistem pendingin pada spot welding sangat berpengaruh terhadap proses pengelasan material kerja yang di las. Media pendingin dan waktu pengelasan menentukan kekuatan tarik dari sambungan las plat baja ST 40. Metode yang digunakan adalah eksperimental pengujian dan pengambilan data pada mesin spot welding dan shear test. Metode kuantitatif dipergunakan untuk mengumpulkan data-data serta pengolahan menggunakan metode deskriptif. Pengujian menggunakan standar ASTM E8. Aliran fluida pendingin dalam proses pengelasan titik secara signifikan mempengaruhi diameter HAZ. Aliran fluida yang lebih cepat meningkatkan transfer panas dari elektroda ke pendingin, membantu menjaga suhu elektroda dan material las di bawah 1.500 ºC, sehingga mengurangi keausan elektroda dan mempertahankan ukuran nugget las yang stabil pada 5,00 mm. Diameter HAZ terendah tercatat pada aliran 5 liter/menit dengan diameter HAZ 8,30 mm, sedangkan tertinggi pada aliran 2 liter/menit dengan diameter 10,43 mm. Pendinginan yang terlalu cepat atau waktu pengelasan yang terlalu singkat dapat menyebabkan sambungan las yang rapuh dan menurunkan tegangan tarik. Sebaliknya, pendinginan yang lebih lambat dengan waktu pengelasan yang tepat menghasilkan kekuatan tarik yang optimal dengan mempertahankan integritas struktural sambungan. Hasil optimal ditemukan pada laju aliran fluida 2 liter/menit pada 5,0 detik dengan tegangan tarik 96,10 Mpa, 3 liter/menit pada 6,0 detik dengan tegangan tarik 104,89 Mpa, 4 liter/menit pada 7,0 detik dengan tegangan tarik 114,00 Mpa dan 5 liter/menit pada 8,0 dan 9,0 detik dengan tegangan tarik 116,72 Mpa dan 125,76 Mpa.

Kata kunci

Jaringan kolaborasi para penulis

40 penulis · 128 tautan kepenulisan bersama · 3 lintas organisasi · menampilkan 40 yang paling banyak terhubung

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • Politeknik Negeri Bali
  • Udayana University
  • Afiliasi tidak diketahui
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama
I Wayan Suma WibawaPoliteknik Negeri Bali5
I Dewa Made Cipta SantosaPoliteknik Negeri Bali4
I Nyoman MeirejekiPoliteknik Negeri Bali3
Made Ardikosa Satrya WibawaPoliteknik Negeri Bali2
I Made Agus PutrawanPoliteknik Negeri Bali2
I Wayan Agus Rantia DanaPoliteknik Negeri Bali2
I Gusti Agung Bagus WirajatiPoliteknik Negeri Bali2
I Nyoman SupartaPoliteknik Negeri Bali2
Anak Agung Gede Pradnyana DiputraPoliteknik Negeri Bali2
Achmad WiboloPoliteknik Negeri Bali1
I Wayan TemajaPoliteknik Negeri Bali1
Made Ery ArsanaPoliteknik Negeri Bali1
M. YusufPoliteknik Negeri Bali1
I Made WidiantaraPoliteknik Negeri Bali1
I Ketut SuartaPoliteknik Negeri Bali1
Anak Agung Putu SwabawaPoliteknik Negeri Bali1
Ni Made ErnawatiUdayana University1
I Gst Lanang Made PurwitaAfiliasi tidak diketahui1
Ayu Dwi YulianthiPoliteknik Negeri Bali1
I G P Fajar Pranadi SudhanaPoliteknik Negeri Bali1
I Gde Agus Jaya SadgunaPoliteknik Negeri Bali1
Anak Agung Ayu Ngurah HarminiPoliteknik Negeri Bali1
Putu Adi SupraptoPoliteknik Negeri Bali1
I Putu Merta AstawaPoliteknik Negeri Bali1
Putu HermawatiPoliteknik Negeri Bali1
I Gusti Ketut AbasanaPoliteknik Negeri Bali1
Anom Adiaksa I MadePoliteknik Negeri Bali1
I Nyoman Gde SangkaPoliteknik Negeri Bali1
I Komang KantunPoliteknik Negeri Bali1
A. A. Gede Pradnyana DiputraPoliteknik Negeri Bali1
I Ketut SuhermanPoliteknik Negeri Bali1
Made Ardikosa Satrya WibawaAfiliasi tidak diketahui1
I Ketut AdiPoliteknik Negeri Bali1
I Made Bagus Panji AdityaPoliteknik Negeri Bali1
Sudirman SudirmanPoliteknik Negeri Bali1
I Made SuginaPoliteknik Negeri Bali1

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OAI-PMH (metadata jurnal) https://ojs2.pnb.ac.id/index.php/JAMETECH/oai, pertama di-harvest 19 Nov 2026, terakhir terlihat 19 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/  http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
	<dc:title xml:lang="en-US">Analisis Pengaruh Aliran Fluida Pendingin dan Waktu Pengelasan Spot Welding Kw14-1031 Terhadap Kekuatan Tarik Pelat Baja ST 40</dc:title>
	<dc:title xml:lang="id-ID">Analisis Pengaruh Aliran Fluida Pendingin Dan Waktu Pengelasan Spot Welding Kw14-1031 Terhadap Kekuatan Tarik Pelat Baja ST 40</dc:title>
	<dc:creator>Adiaksa, I Made Anom </dc:creator>
	<dc:creator>I Nyoman Gede Suta Waisnawa</dc:creator>
	<dc:creator>Ida Bagus Gde Widiantara</dc:creator>
	<dc:creator>I Wayan Marlon Managi</dc:creator>
	<dc:subject xml:lang="en-US">fluid</dc:subject>
	<dc:subject xml:lang="en-US">coolant</dc:subject>
	<dc:subject xml:lang="en-US">spot</dc:subject>
	<dc:subject xml:lang="en-US">welding</dc:subject>
	<dc:subject xml:lang="en-US">strength</dc:subject>
	<dc:subject xml:lang="en-US">tensile</dc:subject>
	<dc:description xml:lang="en-US">Spot welding is greatly influenced by the cooling medium in terms of welding characteristics such as strength. The tensile strength of ST 40 steel plate welded joints is influenced by the cooling medium and welding time. Testing and data collection use experimental methods on spot welding machines and shear tests. Data collection uses quantitative methods while processing uses descriptive methods. The ASTM E8 standard is used in sample testing. The flow of coolant fluid in the spotwelding process significantly affects the HAZ diameter. Faster fluid flow increases heat transfer from the electrode to the coolant, keeping the electrode and weld material temperatures below 1,500 ºC, thereby reducing electrode wear and maintaining a stable weld nugget size at 5.00 mm. The lowest HAZ diameter was recorded at a flow rate of 5 liters/minute with a HAZ diameter of 8.30 mm, while the highest was at a flow rate of 2 liters/minute with a diameter of 10.43 mm. Too fast cooling or too short welding time can cause brittle weld joints and reduce tensile stress. Conversely, slower cooling with appropriate welding time produces optimal tensile strength while maintaining the structural integrity of the joint. Optimal results were found at a fluid flow rate of 2 liters/minute at 5.0 seconds with a tensile stress of 96.10 MPa, 3 liters/minute at 6.0 seconds with a tensile stress of 104.89 MPa, 4 liters/minute at 7.0 seconds with a tensile stress of 114.00 MPa and 5 liters/minute at 8.0 and 9.0 seconds with tensile stress of 116.72 MPa and 125.76 MPa.</dc:description>
	<dc:description xml:lang="id-ID">Media pendingin pada pengelasan ini sangat mempengaruhi karakteristik hasil pengelasan seperti kekuatan. Penempatan sistem pendingin pada spot welding sangat berpengaruh terhadap proses pengelasan material kerja yang di las. Media pendingin dan waktu pengelasan menentukan kekuatan tarik dari sambungan las plat baja ST 40. &amp;nbsp;Metode yang digunakan adalah eksperimental pengujian dan pengambilan data pada mesin spot welding dan shear test. Metode kuantitatif dipergunakan untuk mengumpulkan data-data serta pengolahan menggunakan metode deskriptif. Pengujian menggunakan standar ASTM E8. Aliran fluida pendingin dalam proses pengelasan titik secara signifikan mempengaruhi diameter HAZ. Aliran fluida yang lebih cepat meningkatkan transfer panas dari elektroda ke pendingin, membantu menjaga suhu elektroda dan material las di bawah 1.500 ºC, sehingga mengurangi keausan elektroda dan mempertahankan ukuran nugget las yang stabil pada 5,00 mm. Diameter HAZ terendah tercatat pada aliran 5 liter/menit dengan diameter HAZ 8,30 mm, sedangkan tertinggi pada aliran 2 liter/menit dengan diameter 10,43 mm. Pendinginan yang terlalu cepat atau waktu pengelasan yang terlalu singkat dapat menyebabkan sambungan las yang rapuh dan menurunkan tegangan tarik. Sebaliknya, pendinginan yang lebih lambat dengan waktu pengelasan yang tepat menghasilkan kekuatan tarik yang optimal dengan mempertahankan integritas struktural sambungan. Hasil optimal ditemukan pada laju aliran fluida 2 liter/menit pada 5,0 detik dengan tegangan tarik 96,10 Mpa, 3 liter/menit pada 6,0 detik dengan tegangan tarik 104,89 Mpa, 4 liter/menit pada 7,0 detik dengan tegangan tarik 114,00 Mpa dan 5 liter/menit pada 8,0 dan 9,0 detik dengan tegangan tarik 116,72 Mpa dan 125,76 Mpa.</dc:description>
	<dc:publisher xml:lang="en-US">Unit Publikasi Ilmiah, P3M, Politeknik Negeri Bali</dc:publisher>
	<dc:date>2026-04-24</dc:date>
	<dc:type>info:eu-repo/semantics/article</dc:type>
	<dc:type>info:eu-repo/semantics/publishedVersion</dc:type>
	<dc:type xml:lang="en-US">Peer-reviewed Article</dc:type>
	<dc:format>application/pdf</dc:format>
	<dc:identifier>https://ojs2.pnb.ac.id/index.php/JAMETECH/article/view/2586</dc:identifier>
	<dc:identifier>10.31940/jametech.v4i1.8-13</dc:identifier>
	<dc:source xml:lang="en-US"> Journal of Applied Mechanical Engineering and Green Technology; Vol. 4 No. 1 (2026): April; 8-13</dc:source>
	<dc:source>2684-8201</dc:source>
	<dc:source>2655-9145</dc:source>
	<dc:source>10.31940/jametech.v4i1</dc:source>
	<dc:language>ind</dc:language>
	<dc:relation>https://ojs2.pnb.ac.id/index.php/JAMETECH/article/view/2586/1483</dc:relation>
	<dc:rights xml:lang="en-US">Copyright (c) 2026  Journal of Applied Mechanical Engineering and Green Technology</dc:rights>
	<dc:rights xml:lang="en-US">https://scholar.google.com/citations?hl=en&amp;view_op=list_works&amp;authuser=2&amp;gmla=AJsN-F5k01DNihBDbooUvlNxExv-WhpB3DyY0tjGvHKGcOovATy6tUweEZBP3T70BKOQ_1Vu8vDBsjKH91JWXJ8-wUV3JCO9xIjSPLsxXRi8L5d6dn6VJWk&amp;user=PhqmFRYAAAAJ</dc:rights>
</oai_dc:dc>