Mold Design for Injection Molding Machine Using Recycled Aluminum

Logic: Jurnal Rancang Bangun dan Teknologi · Vol. 25 No. 1 (2025) · hlm. 54–60

DOI
10.31940/logic.v25i1.54-60
ISSN
2580-5649, 1412-114X
Terbit
2025-03-30
Penerbit
Unit Publikasi Ilmiah, P3M, Politeknik Negeri Bali
Bahasa
eng

Abstrak

The use of aluminum is widely spread from beverage cans, car parts, airplanes, trains, and household furniture. This is due to its lightweight and good corrosion resistance. However, as a metal aluminum waste is difficult to be decomposed naturally. Aluminum metal takes 80 to 100 years to decompose. So the accumulation of untreated scrap aluminum can pollute the environment. One of the solutions is to recycle aluminum by melting and re-casting it into a new shape: a mold for polymer processing. The waste of beverage cans was cleaned from any dirt and adhesive. Then, they were turned into small parts by a crusher. The melting process was done at 650oC. The molten aluminum was poured into a sand mould in the shape of mould of a tensile testing specimen. The recycled product can be used to prepare tensile testing samples of polymer or polymer-based composite with injection molding technique. To evaluate the quality of recycled aluminum, a hardness test was done with a value of 69.31 + 3.02 HB. This value is lower than first-use aluminum. This is due to a combination of microstructural changes due to repeated heating, the presence of additives and impurities, and the effects of heat treatment and open cooling. Metallographic testing was carried out to evaluate the microstructure of the material resulting from the smelting of scrap aluminum using sand molds. In this test, the etching solution used consisted of 100 ml of water and 20 g of sodium hydroxide. The results of the metallographic images on the recycled aluminum material show the presence of a stand-alone silicon (Si) element and an aluminum-copper alloy (CuAl₂).

Kata kunci

Jaringan kolaborasi para penulis

36 penulis · 104 tautan kepenulisan bersama · 19 lintas organisasi

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • Politeknik Negeri Bali
  • Sumatera Institute of Technology
  • Universitas Widyatama
  • Universitas Jenderal Achmad Yani
  • Bandung Institute of Technology
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama
I Wayan Padma Yogi AsanaPoliteknik Negeri Bali6
Wahyu Solafide SipahutarSumatera Institute of Technology2
Putu Wijaya SunuPoliteknik Negeri Bali2
I Made SuartaPoliteknik Negeri Bali2
M KusumaPoliteknik Negeri Bali2
Ni Luh Wisma Eka YantiBandung Institute of Technology2
Anisa FitriSumatera Institute of Technology2
Sena MaulanaSumatera Institute of Technology1
Rio Ardiansyah MurdaSumatera Institute of Technology1
Fajar Aditya JulyatmojoSumatera Institute of Technology1
Astri Aulia SuwandaSumatera Institute of Technology1
Muhammad Saeful FadlanSumatera Institute of Technology1
I Wayan TemajaPoliteknik Negeri Bali1
Ida Ayu Anom ArsaniPoliteknik Negeri Bali1
I Gede Artha NegaraPoliteknik Negeri Bali1
I Nyoman Gede BaliartaPoliteknik Negeri Bali1
I Wayan SutinaPoliteknik Negeri Bali1
I Nyoman SupartaPoliteknik Negeri Bali1
I Wayan Suma WibawaPoliteknik Negeri Bali1
I Komang KantunPoliteknik Negeri Bali1
I Ketut SuhermanPoliteknik Negeri Bali1
I Wayan SuiryaPoliteknik Negeri Bali1
I Nyoman GunungPoliteknik Negeri Bali1
Anak Agung Ngurah Bagus MulawarmanPoliteknik Negeri Bali1
I N. G. SastrawanPoliteknik Negeri Bali1
Bagus RadityaPoliteknik Negeri Bali1
Selly SeptianissaUniversitas Widyatama1
Muhamad WaldiUniversitas Jenderal Achmad Yani1
Azizul FikriSumatera Institute of Technology1
Mhd. Yasin SiregarSumatera Institute of Technology1
Faiza Armalia PutriSumatera Institute of Technology1
I Komang RusmariadiPoliteknik Negeri Bali1

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OAI-PMH (metadata jurnal) https://ojs2.pnb.ac.id/index.php/LOGIC/oai, pertama di-harvest 19 Nov 2026, terakhir terlihat 19 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/  http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
	<dc:title xml:lang="en-US">Mold Design for Injection Molding Machine Using Recycled Aluminum</dc:title>
	<dc:creator>Renaldy, Amadeus</dc:creator>
	<dc:creator>Baiti, Risa Nurin </dc:creator>
	<dc:creator>Rahtika, I Putu Gede Sopan</dc:creator>
	<dc:creator>Widantha, Komang Widhi</dc:creator>
	<dc:subject xml:lang="en-US">aluminum</dc:subject>
	<dc:subject xml:lang="en-US">mould</dc:subject>
	<dc:subject xml:lang="en-US">injection moulding</dc:subject>
	<dc:subject xml:lang="en-US">design</dc:subject>
	<dc:subject xml:lang="en-US">recycling</dc:subject>
	<dc:description xml:lang="en-US">The use of aluminum is widely spread from beverage cans, car parts, airplanes, trains, and household furniture. This is due to its lightweight and good corrosion resistance. However, as a metal aluminum waste is difficult to be decomposed naturally. Aluminum metal takes 80 to 100 years to decompose. So the accumulation of untreated scrap aluminum can pollute the environment. One of the solutions is to recycle aluminum by melting and re-casting it into a new shape: a mold for polymer processing. The waste of beverage cans was cleaned from any dirt and adhesive. Then, they were turned into small parts by a crusher. The melting process was done at 650oC. The molten aluminum was poured into a sand mould in the shape of mould of a tensile testing specimen. The recycled product can be used to prepare tensile testing samples of polymer or polymer-based composite with injection molding technique. To evaluate the quality of recycled aluminum, a hardness test was done with a value of 69.31 + 3.02 HB. This value is lower than first-use aluminum. This is due to a combination of microstructural changes due to repeated heating, the presence of additives and impurities, and the effects of heat treatment and open cooling. Metallographic testing was carried out to evaluate the microstructure of the material resulting from the smelting of scrap aluminum using sand molds. In this test, the etching solution used consisted of 100 ml of water and 20 g of sodium hydroxide. The results of the metallographic images on the recycled aluminum material show the presence of a stand-alone silicon (Si) element and an aluminum-copper alloy (CuAl₂).</dc:description>
	<dc:publisher xml:lang="en-US">Unit Publikasi Ilmiah, P3M, Politeknik Negeri Bali</dc:publisher>
	<dc:date>2025-03-30</dc:date>
	<dc:type>info:eu-repo/semantics/article</dc:type>
	<dc:type>info:eu-repo/semantics/publishedVersion</dc:type>
	<dc:format>application/pdf</dc:format>
	<dc:identifier>https://ojs2.pnb.ac.id/index.php/LOGIC/article/view/2452</dc:identifier>
	<dc:identifier>10.31940/logic.v25i1.54-60</dc:identifier>
	<dc:source xml:lang="en-US"> Logic : Jurnal Rancang Bangun dan Teknologi; Vol. 25 No. 1 (2025): March; 54-60</dc:source>
	<dc:source>2580-5649</dc:source>
	<dc:source>1412-114X</dc:source>
	<dc:source>10.31940/logic.v25i1</dc:source>
	<dc:language>eng</dc:language>
	<dc:relation>https://ojs2.pnb.ac.id/index.php/LOGIC/article/view/2452/1101</dc:relation>
	<dc:rights xml:lang="en-US">Copyright (c) 2025  Logic : Jurnal Rancang Bangun dan Teknologi</dc:rights>
	<dc:rights xml:lang="en-US">https://scholar.google.co.id/citations?user=smBuD3gAAAAJ&amp;hl=id</dc:rights>
</oai_dc:dc>