Melola Discovery

← Melola Discovery

Akses terbuka Jurnal SINTA 1

Effect of Immersion Time in Artificial Saliva on Flexural Strength of Provisional Crown and Bridge Material: Light zPolymerization versus Autopolymerization system

Journal of Dentistry Indonesia · Vol. 17 No. 1 (2013)

DOI
10.14693/jdi.v17i1.108
ISSN
1693-9697, 2355-4800
Terbit
2013-07-29
Penerbit
University of Indonesia
Bahasa
en
Lisensi
creativecommons.org/licenses/by/4.0/

Abstrak

Objective: The aim of this study was to investigate the effect of immersion time in artificial salive on the flexural strength of provisional crown and bridge (p-c&b) materials. Materials and Methods: Two types of p-c&b materials were used in this study: Light polymerized p-c&b material (Revotek LC) and autopolymerized p-c&b material (PerfecTemp II). A total of 100 specimens were fabricated and measured according to ISO 4049/2000. A stainless steel mould was used to prepare 2mmx2mmx25mm bar shaped specimens. All materials were dispensed and manipulated according to the manufacturers' instructions. The specimens were divided into 5 groups (n=10). Each specimen of the first group was measured immediately after preparation. The second, third, fourth and fifth groups were immersed in artificial saliva at 37ºC in an incubator for 1 hour, 1 day, 7 days, and 14 days, respectively. Flexural strength was tested by Universal Mechanical Testing Machine Shimadzu in a 3-point bending test. The repeated ANOVA and Post-Hoc Bonferroni test were used to compare the continuous variables between the groups. Results: The results showed flexural strength of Revotek LC were higher than PerfecTemp II at first and second group. However, flexural strength of PerfecTemp II was higher than Revotek LC at third, fourth, and fifth group. The highest flexural strength of Revotek LC was achieved in 1 hour immersion, whereas PerfecTemp II achieved the highest value in 7 days. Conclusion: Flexural strength of p-c&b materials were influenced by immersion time in artifical saliva and the type of p-c&b materials. DOI: 10.14693/jdi.v17i1.108

Kata kunci

Jaringan kolaborasi para penulis

12 penulis · 27 tautan kepenulisan bersama · 2 lintas organisasi

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • University of Indonesia
  • Universitas Syiah Kuala
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama
Yosi Kusuma EriwatiUniversity of Indonesia2
Ferry JayaUniversity of Indonesia1
Andi Soufyan SUniversity of Indonesia1
Anton RahardjoUniversity of Indonesia1
Diah Ayu MaharaniUniversity of Indonesia1
KarinaUniversity of Indonesia1
Adini FadhilahUniversity of Indonesia1
Iin SundariUniversitas Syiah Kuala1
Andi SoufyanUniversity of Indonesia1

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OpenAlex API (jurnal SINTA, ADR 0048) https://openalex.org/S2736430281, pertama di-harvest 19 Nov 2026, terakhir terlihat 19 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/"><dc:title xml:lang="en">Effect of Immersion Time in Artificial Saliva on Flexural Strength of Provisional Crown and Bridge Material: Light zPolymerization versus Autopolymerization system</dc:title><dc:creator>Marzia Magdalena Tetelepta</dc:creator><dc:creator>Bambang Irawan</dc:creator><dc:creator>Siti Triaminingsih</dc:creator><dc:subject>flexural strength</dc:subject><dc:subject>artificial saliva immersion</dc:subject><dc:subject>autopolymerization</dc:subject><dc:subject>immersion time</dc:subject><dc:description xml:lang="en">Objective: The aim of this study was to investigate the effect of immersion time in artificial salive on the flexural strength of provisional crown and bridge (p-c&amp;b) materials. Materials and Methods: Two types of p-c&amp;b materials were used in this study: Light polymerized p-c&amp;b material (Revotek LC) and autopolymerized p-c&amp;b material (PerfecTemp II). A total of 100 specimens were fabricated and measured according to ISO 4049/2000. A stainless steel mould was used to prepare 2mmx2mmx25mm bar shaped specimens. All materials were dispensed and manipulated according to the manufacturers' instructions. The specimens were divided into 5 groups (n=10). Each specimen of the first group was measured immediately after preparation. The second, third, fourth and fifth groups were immersed in artificial saliva at 37ºC in an incubator for 1 hour, 1 day, 7 days, and 14 days, respectively. Flexural strength was tested by Universal Mechanical Testing Machine Shimadzu in a 3-point bending test. The repeated ANOVA and Post-Hoc Bonferroni test were used to compare the continuous variables between the groups. Results: The results showed flexural strength of Revotek LC were higher than PerfecTemp II at first and second group. However, flexural strength of PerfecTemp II was higher than Revotek LC at third, fourth, and fifth group. The highest flexural strength of Revotek LC was achieved in 1 hour immersion, whereas PerfecTemp II achieved the highest value in 7 days. Conclusion: Flexural strength of p-c&amp;b materials were influenced by immersion time in artifical saliva and the type of p-c&amp;b materials. DOI: 10.14693/jdi.v17i1.108</dc:description><dc:publisher>University of Indonesia</dc:publisher><dc:date>2013-07-29</dc:date><dc:type>info:eu-repo/semantics/article</dc:type><dc:identifier>https://doi.org/10.14693/jdi.v17i1.108</dc:identifier><dc:identifier>10.14693/jdi.v17i1.108</dc:identifier><dc:source>Journal of Dentistry Indonesia; Vol 17 No 1 (2013)</dc:source><dc:source>1693-9697</dc:source><dc:source>2355-4800</dc:source><dc:language>en</dc:language><dc:rights>https://creativecommons.org/licenses/by/4.0/</dc:rights></oai_dc:dc>