Melola Discovery

← Melola Discovery

Jurnal Tanpa peringkat SINTA

The Shear Bond and Bending Strength of Laminated Wood From Pine Wood (Pinus merkusii Jungh et de Vr.,) and Sengon Wood (Paraserianthes falcataria (L) Nielsen) Glued With Melamine Urea Formaldehyde (MUF): Keteguhan Rekat Geser dan Keteguhan Lengkung Statis Kayu Laminasi dari Kayu Pinus (Pinus merkusii Jungh et de Vr.) dan Kayu Sengon (Paraserianthes falcataria (L) Nielsen) Berperekat Melamins Urea Formaldehida (MUF)

Keteguhan Rekat Geser dan Keteguhan Lengkung Statis Kayu Laminasi dari Kayu Pinus (Pinus merkusii Jungh et de Vr.) dan Kayu Sengon (Paraserianthes falcataria (L) Nielsen) Berperekat Melamins Urea Formaldehida (MUF): The Shear Bond and Bending Strength of Laminated Wood From Pine Wood (Pinus merkusii Jungh et de Vr.,) and Sengon Wood (Paraserianthes falcataria (L) Nielsen) Glued With Melamine Urea Formaldehyde (MUF)

PERENNIAL · Vol. 20 No. 1 (2024) · hlm. 1–10

DOI
10.24259/perennial.v20i1.33966
ISSN
2685-6859, 1412-7784
Terbit
2024-04-30
Penerbit
Forestry Faculty of Hasanuddin University
Bahasa
en

Abstrak

Inggris

Laminated wood's strength properties are influenced by the arrangement of each layers. This research aims to determine the effect of variations in layers of laminated wood to the shear bond strength, modulus of elasticity (MoE) and modulus of rupture (MoR) of laminated wood from Pine (P) and Sengon (S) wood using melamine urea formaldehyde adhesive (MUF). Laminated wood is tested using German standards DIN (Deutsches Intitut fur Normung), JAS 234-2007 and SNI 7973-2013. The data testing from 6 layer variation treatments were analyzed of variance in a completely randomized design (CRD) with 10 replications. The highest average value of shear bond strength for laminated wood in treatment G2 (Sengon-Sengon) was 6.17 N/mm2 which met the JAS 234-2007 standard (>5.4 N/mm2) while treatment G3 (Pine-Sengon) was 4.04 N/mm2 and G1 (Pine-Pine) of 2.78 N/mm2 cannot meet the standard. The highest average MoE was at A5 (P-S-S-P-P) at 8584.27 N/mm2 and the lowest at A3 (P-S-P) at 6210.99 N/mm2 included quality codes E8 and E6 in the SNI 7973-2013 Standard. The highest average MoR was at A4 (P-S-S-S-P) at 73.23 N/mm2 and the lowest at A5 (P-S-S-P-P) at 61.98 N/mm2, all treatments included quality code E25 (>25 N/mm2) and could meet JAS 234-2007 Standards (>36.0 N/mm2). The laminated wood in this study based on MoR is included to the strength class III – II and located between the strength class of Pine wood (strength class II) and Sengon wood (strength class III).

Bahasa Indonesia

Kayu laminasi sifat kekuatannya sangat dipengaruhi oleh penyusunan tiap lapisannya. Penelitian ini bertujuan mengetahui pengaruh variasi lapisan kayu laminasi terhadap keteguhan rekat geser, modulus elastisitas (MoE) dan keteguhan patah (MoR) kayu laminasi dari jenis kayu Pinus (P) dan kayu Sengon (S) menggunakan perekat melamin urea formaldehid (MUF). Kayu lamina diuji menggunakan standar Jerman DIN, JAS 234-2007 dan SNI 7973-2013. Data pengujian 6 perlakuan variasi lapisan dianalisis keragaman dalam rancangan acak lengkap (RAL) dengan 10 ulangan. Rataan keteguhan rekat geser kayu lamina tertinggi pada perlakuan G2 (Sengon-Sengon) sebesar 6.17 N/mm2 dapat memenuhi standar JAS 234-2007 (>5.4 N/mm2) sedangkan perlakuan G3 (Pinus-Sengon) sebesar 4.04 N/mm2 dan G1 (Pinus-Pinus) sebesar 2.78 N/mm2 tidak dapat memenuhi standar. Rataan MoE tertinggi pada A5 (P-S-S-P-P) sebesar 8584.27 N/mm2 dan terendah pada A3 (P-S-P) sebesar 6210.99 N/mm2 termasuk kode mutu E8 dan E6 pada Standar SNI 7973-2013. Rataan MoR tertinggi pada A4 (P-S-S-S-P) sebesar 73.23 N/mm2 dan terendah pada A5 (P-S-S-P-P) sebesar 61.98 N/mm2, semua perlakuan termasuk kode mutu E25 (>25 N/mm2) dan dapat memenuhi standar JAS 234-2007 (>36.0 N/mm2). Kayu laminasi dalam penelitian ini berdasarkan MoR termasuk kelas kuat III – II dan terletak diantara kelas kuat kayu Pinus (kelas kuat II) dan kayu Sengon (kelas kuat III).

Kata kunci

Jaringan kolaborasi para penulis

2 penulis · 1 tautan kepenulisan bersama

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • Mulawarman University
  • Afiliasi tidak diketahui
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama
IRVIN DAYADIAfiliasi tidak diketahui1

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OAI-PMH (metadata jurnal) https://journal.unhas.ac.id/index.php/perennial/oai, pertama di-harvest 5 Nov 2026, terakhir terlihat 15 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/  http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
	<dc:title xml:lang="en">The Shear Bond and Bending Strength of Laminated Wood From Pine Wood (Pinus merkusii Jungh et de Vr.,) and Sengon Wood (Paraserianthes falcataria (L) Nielsen) Glued With Melamine Urea Formaldehyde (MUF):  Keteguhan Rekat Geser dan Keteguhan Lengkung Statis Kayu Laminasi dari Kayu Pinus (Pinus merkusii Jungh et de Vr.) dan Kayu Sengon (Paraserianthes falcataria (L) Nielsen) Berperekat Melamins Urea Formaldehida (MUF)</dc:title>
	<dc:title xml:lang="id"> Keteguhan Rekat Geser dan Keteguhan Lengkung Statis Kayu Laminasi dari Kayu Pinus (Pinus merkusii Jungh et de Vr.) dan Kayu Sengon (Paraserianthes falcataria (L) Nielsen) Berperekat Melamins Urea Formaldehida (MUF): The Shear Bond and Bending Strength of Laminated Wood From Pine Wood (Pinus merkusii Jungh et de Vr.,) and Sengon Wood (Paraserianthes falcataria (L) Nielsen) Glued With Melamine Urea Formaldehyde (MUF)</dc:title>
	<dc:creator xml:lang="en">DAYADI, IRVIN</dc:creator>
	<dc:subject xml:lang="id">Kayu laminasi</dc:subject>
	<dc:subject xml:lang="id">Melamin formaldehida</dc:subject>
	<dc:subject xml:lang="id">Pinus</dc:subject>
	<dc:subject xml:lang="id">Sengon</dc:subject>
	<dc:subject xml:lang="id">Variasi lapisan</dc:subject>
	<dc:subject xml:lang="en">Laminated wood</dc:subject>
	<dc:subject xml:lang="en">Melamine formaldehide</dc:subject>
	<dc:subject xml:lang="en">Pine</dc:subject>
	<dc:subject xml:lang="en">Sengon</dc:subject>
	<dc:subject xml:lang="en">Variations in layers</dc:subject>
	<dc:description xml:lang="en">



Laminated wood's strength properties are influenced by the arrangement of each layers. This research aims to determine the effect of variations in layers of laminated wood to the shear bond strength, modulus of elasticity (MoE) and modulus of rupture (MoR) of laminated wood from Pine (P) and Sengon (S) wood using melamine urea formaldehyde adhesive (MUF). Laminated wood is tested using German standards DIN (Deutsches Intitut fur Normung), JAS 234-2007 and SNI 7973-2013. The data testing from 6 layer variation treatments were analyzed of variance in a completely randomized design (CRD) with 10 replications. The highest average value of shear bond strength for laminated wood in treatment G2 (Sengon-Sengon) was 6.17 N/mm2 which met the JAS 234-2007 standard (&amp;gt;5.4 N/mm2) while treatment G3 (Pine-Sengon) was 4.04 N/mm2 and G1 (Pine-Pine) of 2.78 N/mm2 cannot meet the standard. The highest average MoE was at A5 (P-S-S-P-P) at 8584.27 N/mm2 and the lowest at A3 (P-S-P) at 6210.99 N/mm2 included quality codes E8 and E6 in the SNI 7973-2013 Standard. The highest average MoR was at A4 (P-S-S-S-P) at 73.23 N/mm2 and the lowest at A5 (P-S-S-P-P) at 61.98 N/mm2, all treatments included quality code E25 (&amp;gt;25 N/mm2) and could meet JAS 234-2007 Standards (&amp;gt;36.0 N/mm2). The laminated wood in this study based on MoR is included to the strength class III – II and located between the strength class of Pine wood (strength class II) and Sengon wood (strength class III).




 
 </dc:description>
	<dc:description xml:lang="id">



Kayu laminasi sifat kekuatannya sangat dipengaruhi oleh penyusunan tiap lapisannya. Penelitian ini bertujuan mengetahui pengaruh variasi lapisan kayu laminasi terhadap keteguhan rekat geser, modulus elastisitas (MoE) dan keteguhan patah (MoR) kayu laminasi dari jenis kayu Pinus (P) dan kayu Sengon (S) menggunakan perekat melamin urea formaldehid (MUF). Kayu lamina diuji menggunakan standar Jerman DIN, JAS 234-2007 dan SNI 7973-2013. Data pengujian 6 perlakuan variasi lapisan dianalisis keragaman dalam rancangan acak lengkap (RAL) dengan 10 ulangan. Rataan keteguhan rekat geser kayu lamina tertinggi pada perlakuan G2 (Sengon-Sengon) sebesar 6.17 N/mm2 dapat memenuhi standar JAS 234-2007 (&amp;gt;5.4 N/mm2) sedangkan perlakuan G3 (Pinus-Sengon) sebesar 4.04 N/mm2 dan G1 (Pinus-Pinus) sebesar 2.78 N/mm2 tidak dapat memenuhi standar. Rataan MoE tertinggi pada A5 (P-S-S-P-P) sebesar 8584.27 N/mm2 dan terendah pada A3 (P-S-P) sebesar 6210.99 N/mm2 termasuk kode mutu E8 dan E6 pada Standar SNI 7973-2013. Rataan MoR tertinggi pada A4 (P-S-S-S-P) sebesar 73.23 N/mm2 dan terendah pada A5 (P-S-S-P-P) sebesar 61.98 N/mm2,  semua perlakuan termasuk kode mutu E25 (&amp;gt;25 N/mm2) dan dapat memenuhi standar JAS 234-2007 (&amp;gt;36.0 N/mm2). Kayu laminasi dalam penelitian ini berdasarkan MoR termasuk kelas kuat III – II dan terletak diantara kelas kuat kayu Pinus (kelas kuat II) dan kayu Sengon (kelas kuat III).



</dc:description>
	<dc:publisher xml:lang="en">Forestry Faculty of Hasanuddin University</dc:publisher>
	<dc:date>2024-04-30</dc:date>
	<dc:type>info:eu-repo/semantics/article</dc:type>
	<dc:type>info:eu-repo/semantics/publishedVersion</dc:type>
	<dc:type xml:lang="en">Peer-reviewed Article</dc:type>
	<dc:format>application/pdf</dc:format>
	<dc:format>application/pdf</dc:format>
	<dc:identifier>https://journal.unhas.ac.id/index.php/perennial/article/view/33966</dc:identifier>
	<dc:identifier>10.24259/perennial.v20i1.33966</dc:identifier>
	<dc:source xml:lang="en">PERENNIAL; Vol. 20 No. 1 (2024): Vol. 20 No. 1, April 2024; 1-10</dc:source>
	<dc:source xml:lang="id">PERENNIAL; Vol 20 No 1 (2024): Vol. 20 No. 1, April 2024; 1-10</dc:source>
	<dc:source>2685-6859</dc:source>
	<dc:source>1412-7784</dc:source>
	<dc:language>en</dc:language>
	<dc:language>id</dc:language>
	<dc:relation>https://journal.unhas.ac.id/index.php/perennial/article/view/33966/11453</dc:relation>
	<dc:relation>https://journal.unhas.ac.id/index.php/perennial/article/view/33966/11452</dc:relation>
</oai_dc:dc>