Melola Discovery

← Melola Discovery

Open access Jurnal SINTA 1

Effect of Na-EDTA on electrical characteristics NaCl electrolyte battery charging solar panels

International Journal of Electrical and Computer Engineering (IJECE) · Vol. 14 No. 5 (2024)

DOI
10.11591/ijece.v14i5.pp4846-4855
ISSN
2722-2578, 2088-8708
Published
2024-10-01
Publisher
Institute of Advanced Engineering and Science
License
creativecommons.org/licenses/by-sa/4.0

Abstract

This research investigates the problem of Cu-Zn electrode batteries with NaCl electrolyte. Previous studies have indicated problems with the electrolyte and electrodes after charging, such as turbidity and deposits in the electrolyte, as well as corrosion on the electrodes. Consequently, the battery can only be used once due to a decline in its electrical characteristics after the initial charging. Through this research, improvements were made to the electrical characteristics of the battery by adding Na-EDTA to enhance usage efficiency. The research method involved mixing NaCl solution with the highest electrical conductivity, using six pairs of Cu-Zn electrodes arranged in series. The physical conditions of the electrolyte and electrodes were observed, and electrical characteristics were measured. The research results indicate that the use of NaCl+Na-EDTA electrolyte produces a battery voltage of 4.20 volts with a current of 2 Ah and can be used twice. Charging with solar panels can be done in 1 hour, but the frequency is limited to two times.

Collaboration network of the authors

9 authors · 24 co-authorship links · 8 across different organisations

Hover or tap a name to highlight its co-authors. Double-click to open the author's page.

  • Medan Area University
  • Andalas University
  • Different organisations
  • Same organisation
  • Affiliation unknown
  • Thicker line = more joint articles · bigger circle = more articles
Show as table
Co-authorOrganisationJoint articles
Indri DayanaMedan Area University4
Dadan RamdanMedan Area University4
Rahmad SyahMedan Area University2
Nukhe Andri SilvianaMedan Area University2

Affiliations come from OpenAlex; journal OAI-PMH metadata carries none. Authors without an OpenAlex ID are matched by name, which can merge or split people.

This record comes from Crossref (what the publisher deposited), because the journal's own OAI-PMH endpoint could not be harvested.

Metadata source: Crossref API (cadangan, berdasarkan ISSN) https://api.crossref.org/journals/2088-8708/works, first harvested 27 Okt 2026, last seen 27 Okt 2026.
Metadata as oai_dc, converted from Crossref
<oai_dc:dc xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/"><dc:title>Effect of Na-EDTA on electrical characteristics NaCl electrolyte battery charging solar panels</dc:title><dc:creator>Maizana, Dina</dc:creator><dc:creator>Mungkin, Moranain</dc:creator><dc:creator>Satria, Habib</dc:creator><dc:creator>Syafii, Syafii</dc:creator><dc:creator>Siregar, Muhammad Fadlan</dc:creator><dc:description>&lt;jats:p&gt;This research investigates the problem of Cu-Zn electrode batteries with NaCl electrolyte. Previous studies have indicated problems with the electrolyte and electrodes after charging, such as turbidity and deposits in the electrolyte, as well as corrosion on the electrodes. Consequently, the battery can only be used once due to a decline in its electrical characteristics after the initial charging. Through this research, improvements were made to the electrical characteristics of the battery by adding Na-EDTA to enhance usage efficiency. The research method involved mixing NaCl solution with the highest electrical conductivity, using six pairs of Cu-Zn electrodes arranged in series. The physical conditions of the electrolyte and electrodes were observed, and electrical characteristics were measured. The research results indicate that the use of NaCl+Na-EDTA electrolyte produces a battery voltage of 4.20 volts with a current of 2 Ah and can be used twice. Charging with solar panels can be done in 1 hour, but the frequency is limited to two times.&lt;/jats:p&gt;</dc:description><dc:publisher>Institute of Advanced Engineering and Science</dc:publisher><dc:date>2024-10-01</dc:date><dc:type>info:eu-repo/semantics/article</dc:type><dc:format>application/pdf</dc:format><dc:identifier>https://doi.org/10.11591/ijece.v14i5.pp4846-4855</dc:identifier><dc:identifier>10.11591/ijece.v14i5.pp4846-4855</dc:identifier><dc:source>International Journal of Electrical and Computer Engineering (IJECE); Vol 14 No 5 (2024); 4846</dc:source><dc:source>2722-2578</dc:source><dc:source>2088-8708</dc:source><dc:relation>https://ijece.iaescore.com/index.php/IJECE/article/viewFile/35337/17625</dc:relation><dc:rights>http://creativecommons.org/licenses/by-sa/4.0</dc:rights></oai_dc:dc>