Abstract

Degradation of Methanil yellow has been done. In this research the degradation process was done by sunlighting and using TiO2-SnO2 catalysis. The residu of methanil yellow was centrifuged and measured by UV/Vis Spectrophotometer at 300 – 600 nm after degradation. 6 mg/L of Methanil yellow and addition of 0,03 g TiO2-SnO2 for 150 min, gave the percentage of degradation 98,413% after lighted by sun with 1,13256 1015 foton cm-2/s intensity.

Keywords

Collaboration network of the authors

40 authors · 115 co-authorship links · 8 across different organisations · showing the 40 most connected

Hover or tap a name to highlight its co-authors. Double-click to open the author's page.

  • Andalas University
  • Universitas Islam Negeri Ar-Raniry
  • University of Indonesia
  • Affiliation unknown
  • Different organisations
  • Same organisation
  • Affiliation unknown
  • Thicker line = more joint articles · bigger circle = more articles
Show as table
Co-authorOrganisationJoint articles
Diana Vanda WelliaAndalas University4
Upita SeptianiAndalas University4
Novesar JamarunAndalas University3
Mai EfdiAndalas University2
Yulia Eka PutriAndalas University2
Reza Audina PutriAndalas University2
Deswati DeswatiAndalas University2
Hamzar SuyaniAndalas University2
Anjar Purba AsmaraUniversitas Islam Negeri Ar-Raniry1
Nurhayati NurhayatiUniversitas Islam Negeri Ar-Raniry1
S BelliaUniversitas Islam Negeri Ar-Raniry1
Febrina ArfiUniversitas Islam Negeri Ar-Raniry1
Zaimi AbdullahAndalas University1
Trisna OllinovelaAffiliation unknown1
Eno Okta PatriciaAndalas University1
Yulizar YusufAndalas University1
Kevin SeptiogaAndalas University1
Syukri AriefAndalas University1
Nofebriani DinaAndalas University1
Nurul PratiwiAndalas University1
Fadhil FerdianAndalas University1
Yetria RildaAndalas University1
Yuli Okta FitriyaniAndalas University1
Emriadi EmriadiAndalas University1
Fitria RamadhaniAndalas University1
Hermansyah AzizAndalas University1
Hazanita JumiatyAndalas University1
Jarnuzi GunlazuardiUniversity of Indonesia1
Khoiriah KhoiriahAndalas University1
Zilfa ZilfaAndalas University1
Vivi SiscaAndalas University1
Aju DeskaAndalas University1
Hilfi PardiAndalas University1
Umiati LoekmanAndalas University1
Wulandari WulandariAndalas University1
Tri Yupi AmirullahAndalas University1
Arika PrasejatiAndalas University1

Affiliations come from OpenAlex; journal OAI-PMH metadata carries none. Authors without an OpenAlex ID are matched by name, which can merge or split people.

Metadata source: OAI-PMH (metadata jurnal) https://jurnal.ar-raniry.ac.id/index.php/lantanida/oai, first harvested 7 Nov 2026, last seen 7 Nov 2026.
Original metadata (oai_dc)
<oai_dc:dc xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/  http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
	<dc:title xml:lang="en">DEGRADASI ZAT WARNA METANIL YELLOW DENGAN PENYINARAN MATAHARI DAN PENAMBAHAN KATALIS TiO2-SnO2</dc:title>
	<dc:creator xml:lang="en">Gita Bhernama, Bhayu</dc:creator>
	<dc:creator xml:lang="en">Safni, Safni</dc:creator>
	<dc:creator xml:lang="en">Syukri, Syukri</dc:creator>
	<dc:subject xml:lang="en">Methanil Yellow</dc:subject>
	<dc:subject xml:lang="en">Sunlighting</dc:subject>
	<dc:subject xml:lang="en">TiO2-SnO2 Catalysis.</dc:subject>
	<dc:description xml:lang="en">Degradation of Methanil yellow has been done. In this research the degradation process was done by sunlighting and using TiO2-SnO2 catalysis. The residu of methanil yellow was centrifuged and measured by UV/Vis Spectrophotometer at   300 – 600 nm after degradation. 6 mg/L of Methanil yellow and addition of 0,03 g TiO2-SnO2 for 150 min, gave the percentage of degradation 98,413% after lighted by sun with 1,13256 1015 foton cm-2/s intensity.</dc:description>
	<dc:publisher xml:lang="en">UIN AR-RANIRY</dc:publisher>
	<dc:date>2017-09-15</dc:date>
	<dc:type>info:eu-repo/semantics/article</dc:type>
	<dc:type>info:eu-repo/semantics/publishedVersion</dc:type>
	<dc:type xml:lang="en">Peer-reviewed Article</dc:type>
	<dc:format>application/pdf</dc:format>
	<dc:identifier>https://jurnal.ar-raniry.ac.id/index.php/lantanida/article/view/1653</dc:identifier>
	<dc:identifier>10.22373/lj.v3i2.1653</dc:identifier>
	<dc:source xml:lang="en">Lantanida Journal; Vol. 3 No. 2 (2015); 116-126</dc:source>
	<dc:source xml:lang="id">Lantanida Journal; Vol 3 No 2 (2015); 116-126</dc:source>
	<dc:source>2548-9062</dc:source>
	<dc:source>2356-3133</dc:source>
	<dc:language>eng</dc:language>
	<dc:relation>https://jurnal.ar-raniry.ac.id/index.php/lantanida/article/view/1653/1205</dc:relation>
	<dc:rights xml:lang="en">Copyright (c) 2017 Bhayu Gita Bhernama, Safni Safni, Syukri Syukri</dc:rights>
</oai_dc:dc>