Melola Discovery

← Melola Discovery

Open access Journal SINTA 1

Monitoring Low-Cycle Fatigue Material-Degradation by Ultrasonic Methods

Atom Indonesia · Vol. 36 No. 2 (2011) · pp. 63–68

DOI
10.17146/aij.2010.26
ISSN
2356-5322, 0126-1568
Published
2011-09-08
Publisher
National Research and Innovation Agency
Language
eng
License
creativecommons.org/licenses/by-nc-sa/4.0

Abstract

Any system consisting of structural material often undergoes fatigue, which is caused by dynamic load cycle. As a structural system, nuclear power plant is very likely to have low-cycle fatigue at many of its components. Taking into account the importance of monitoring low-cycle fatigue on structural components to prevent them from getting failure, the authors have conducted a work to monitor material degradation caused by low-cycle fatigue by using ultrasonic method. An alloy of Cu-40Zn was used as a test specimen. Ultrasonic water immersion procedure was employed in this ultrasonic test. The probe used is a focusing type and has frequency as high as 15 MHz. The specimen area tested is in the middle part divided into 14 points × 23 points. The results, which were frequency spectrums, were analyzed using two parameters: frequency spectrum peak intensity and attenuation function gradient. The analysis indicates that peak intensity increases at the beginning of load cycle and then decreases. Meanwhile, gradient of attenuation function is lower at the beginning of fatigue process, and then consistently gets higher. It concludes that low-fatigue material degradation can be monitored by using ultrasonic method.Received: 20 November 2009; Revised: 31 August 2010; Accepted: 31 August 2010

Keywords

Collaboration network of the authors

3 authors · 3 co-authorship links · 2 across different organisations

Hover or tap a name to highlight its co-authors. Double-click to open the author's page.

  • National Nuclear Energy Agency of Indonesia
  • Saitama University
  • Different organisations
  • Same organisation
  • Affiliation unknown
  • Thicker line = more joint articles · bigger circle = more articles
Show as table
Co-authorOrganisationJoint articles

Affiliations come from OpenAlex; journal OAI-PMH metadata carries none. Authors without an OpenAlex ID are matched by name, which can merge or split people.

Metadata source: OAI-PMH (metadata jurnal) https://atomindonesia.brin.go.id/index.php/aij/oai, first harvested 8 Nov 2026, last seen 22 Nov 2026.
Original metadata (oai_dc)
<oai_dc:dc xmlns="http://www.openarchives.org/OAI/2.0/" xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/" xmlns:xsi="http://www.w3.org/2001/XMLSchema-instance" xsi:schemaLocation="http://www.openarchives.org/OAI/2.0/oai_dc/  http://www.openarchives.org/OAI/2.0/oai_dc.xsd">
	<dc:title xml:lang="en-US">Monitoring Low-Cycle Fatigue Material-Degradation by Ultrasonic Methods</dc:title>
	<dc:creator>Himawan, R.</dc:creator>
	<dc:creator>Katoh, H.</dc:creator>
	<dc:creator>Cahyono, A.</dc:creator>
	<dc:subject xml:lang="en-US">Low-cycle fatigue; Non-destructive test;  Ultrasonic method</dc:subject>
	<dc:description xml:lang="en-US">Any system consisting of structural material often undergoes fatigue, which is caused by dynamic load cycle. As a structural system, nuclear power plant is very likely to have low-cycle fatigue at many of its components. Taking into account the importance of monitoring low-cycle fatigue on structural components to prevent them from getting failure, the authors have conducted a work to monitor material degradation caused by low-cycle fatigue by using ultrasonic method. An alloy of Cu-40Zn was used as a test specimen. Ultrasonic water immersion procedure was employed in this ultrasonic test. The probe used is a focusing type and has frequency as high as 15 MHz. The specimen area tested is in the middle part divided into 14 points × 23 points. The results, which were frequency spectrums, were analyzed using two parameters: frequency spectrum peak intensity and attenuation function gradient. The analysis indicates that peak intensity increases at the beginning of load cycle and then decreases. Meanwhile, gradient of attenuation function is lower at the beginning of fatigue process, and then consistently gets higher. It concludes that low-fatigue material degradation can be monitored by using ultrasonic method.Received: 20 November 2009; Revised: 31 August 2010; Accepted: 31 August 2010</dc:description>
	<dc:publisher xml:lang="en-US">National Research and Innovation Agency</dc:publisher>
	<dc:contributor xml:lang="en-US">National Nuclear Energy Agency of Indonesia</dc:contributor>
	<dc:date>2011-09-08</dc:date>
	<dc:type>info:eu-repo/semantics/article</dc:type>
	<dc:type>info:eu-repo/semantics/publishedVersion</dc:type>
	<dc:type xml:lang="en-US"></dc:type>
	<dc:format>application/pdf</dc:format>
	<dc:identifier>https://atomindonesia.brin.go.id/index.php/aij/article/view/26</dc:identifier>
	<dc:identifier>10.17146/aij.2010.26</dc:identifier>
	<dc:source xml:lang="en-US">Atom Indonesia; Vol 36, No 2 (2010): August 2010; 63-68</dc:source>
	<dc:source>2356-5322</dc:source>
	<dc:source>0126-1568</dc:source>
	<dc:source>10.17146/aij.2010.%x</dc:source>
	<dc:language>eng</dc:language>
	<dc:relation>https://atomindonesia.brin.go.id/index.php/aij/article/view/26/18</dc:relation>
	<dc:rights xml:lang="en-US">Copyright (c) 2016 Atom Indonesia</dc:rights>
	<dc:rights xml:lang="en-US">http://creativecommons.org/licenses/by-nc-sa/4.0</dc:rights>
</oai_dc:dc>