Deactivation and Regeneration of Ni/ZA Catalyst in Hydrocracking of Polypropylene

Indonesian Journal of Chemistry · Vol. 14 No. 2 (2014) · hlm. 192–198

DOI
10.22146/ijc.21258
ISSN
1411-9420, 2460-1578
Terbit
2014-07-25
Penerbit
Gadjah Mada University
Bahasa
en
Lisensi
creativecommons.org/licenses/by-nc-nd/4.0/

Abstrak

The phenomena of catalyst deactivation and the effects of regeneration method on the characteristics and activity of Ni/ZA catalyst after being used in a continuous cracking reaction of polypropylene have been studied. Ni/ZA catalyst was prepared using sonochemical method with total metal intake of 4%. Characteristics and activity of fresh, spent, and regenerated catalyst were evaluated to get a better understanding about the catalyst deactivation. Characteristics which have been observed include catalyst acidity, porosity, crystallinity, and surface morphology. Catalytic activity test of Ni/ZA catalyst on polypropylene cracking reaction at temperature of 500 °C with H2 flow rate of 20 mL/min and catalyst:feed ratio of 1:2 (w/w) showed the decrease of some catalyst characteristics such as specific surface area, total pore volume, and acidity due to coke fouling over a five-times continuous experiment. Regeneration of catalyst with oxidation-reduction method has been able to increase the activity and acidity of catalyst up to 7.47% and 38.54%, respectively, compared to those of spent catalyst, while the catalyst surface area and total pore volume decreased up to 32.83% and 26.92%, respectively.

Kata kunci

Jaringan kolaborasi para penulis

40 penulis · 117 tautan kepenulisan bersama · 18 lintas organisasi · menampilkan 40 yang paling banyak terhubung

Arahkan kursor atau ketuk sebuah nama untuk menyorot rekan penulisnya. Klik dua kali untuk membuka halaman penulis.

  • State University of Semarang
  • Indonesia University of Education
  • Hasanuddin University
  • Universitas Gadjah Mada
  • State University of Makassar
  • Institut Teknologi Sepuluh Nopember
  • Kementerian Energi dan Sumber Daya Mineral
  • Organisasi lain
  • Afiliasi tidak diketahui
  • Organisasi berbeda
  • Organisasi sama
  • Afiliasi tidak diketahui
  • Garis lebih tebal = lebih banyak artikel bersama · lingkaran lebih besar = lebih banyak artikel
Tampilkan sebagai tabel
Rekan penulisOrganisasiArtikel bersama
Woro SumarniState University of Semarang3
Fitri RahmawatiIndonesia University of Education2
SRI WAHYUNIHasanuddin University2
Sigit PriatmokoState University of Semarang2
Indriana KartiniUniversitas Gadjah Mada2
Sri Susilogati SumartiState University of Semarang1
Ramlawati RamlawatiState University of Makassar1
Endang SusilaningsihState University of Semarang1
Murbangun NuswowatiState University of Semarang1
Dyah Rini IndriyantiState University of Semarang1
Imas IstianiState University of Semarang1
Muzakki BashoriState University of Semarang1
Maria Ayu PuspitaAfiliasi tidak diketahui1
Novie Prasetyo UtomoAfiliasi tidak diketahui1
Muhammad JaeniAfiliasi tidak diketahui1
Ahmad BurhanudinAfiliasi tidak diketahui1
Eros Meiliana ShofaAfiliasi tidak diketahui1
Muhlisin MuhlisinAfiliasi tidak diketahui1
Ina AnggreaniAfiliasi tidak diketahui1
Woro SumarniState University of Semarang1
Khaerur RifqiAfiliasi tidak diketahui1
Pertiwi Ayu Pamuji KurniatunAfiliasi tidak diketahui1
Harjito HarjitoAfiliasi tidak diketahui1
Lailatul BadriyahAfiliasi tidak diketahui1
Soeprodjo SoeprodjoAfiliasi tidak diketahui1
Luluk Amnah FitriyanaAfiliasi tidak diketahui1
Puji Eka RahayuAfiliasi tidak diketahui1
Harjono HarjonoState University of Semarang1
Samhasari Desthi MuslimahState University of Semarang1
Viqhi AswieInstitut Teknologi Sepuluh Nopember1
Wara Dyah Pita RenggaState University of Semarang1
Prima Astuti HandayaniState University of Semarang1
Agung FeinnudinKementerian Energi dan Sumber Daya Mineral1
Retno Sri IswariState University of Semarang1
R. SusantiState University of Semarang1
Adid Adep DwiatmokoNational Research and Innovation Agency1
Suhailah Salma MaulidaState University of Semarang1

Afiliasi berasal dari OpenAlex; metadata OAI-PMH jurnal tidak memuatnya. Penulis tanpa ID OpenAlex dicocokkan berdasarkan nama, sehingga dua orang bisa tergabung atau satu orang bisa terpisah.

Sumber metadata: OpenAlex API (jurnal SINTA, ADR 0048) https://openalex.org/S2764840418, pertama di-harvest 19 Nov 2026, terakhir terlihat 22 Nov 2026.
Metadata asli (oai_dc)
<oai_dc:dc xmlns:dc="http://purl.org/dc/elements/1.1/" xmlns:oai_dc="http://www.openarchives.org/OAI/2.0/oai_dc/"><dc:title xml:lang="en">Deactivation and Regeneration of Ni/ZA Catalyst in Hydrocracking of Polypropylene</dc:title><dc:creator>Imam Khabib</dc:creator><dc:creator>Sri Kadarwati</dc:creator><dc:creator>Sri Wahyuni</dc:creator><dc:subject>catalyst deactivation</dc:subject><dc:subject>catalyst regeneration</dc:subject><dc:subject>coke formation</dc:subject><dc:subject>catalyst acidity</dc:subject><dc:subject>catalyst porosity</dc:subject><dc:subject>nickel catalysts</dc:subject><dc:description xml:lang="en">The phenomena of catalyst deactivation and the effects of regeneration method on the characteristics and activity of Ni/ZA catalyst after being used in a continuous cracking reaction of polypropylene have been studied. Ni/ZA catalyst was prepared using sonochemical method with total metal intake of 4%. Characteristics and activity of fresh, spent, and regenerated catalyst were evaluated to get a better understanding about the catalyst deactivation. Characteristics which have been observed include catalyst acidity, porosity, crystallinity, and surface morphology. Catalytic activity test of Ni/ZA catalyst on polypropylene cracking reaction at temperature of 500 °C with H2 flow rate of 20 mL/min and catalyst:feed ratio of 1:2 (w/w) showed the decrease of some catalyst characteristics such as specific surface area, total pore volume, and acidity due to coke fouling over a five-times continuous experiment. Regeneration of catalyst with oxidation-reduction method has been able to increase the activity and acidity of catalyst up to 7.47% and 38.54%, respectively, compared to those of spent catalyst, while the catalyst surface area and total pore volume decreased up to 32.83% and 26.92%, respectively.</dc:description><dc:publisher>Gadjah Mada University</dc:publisher><dc:date>2014-07-25</dc:date><dc:type>info:eu-repo/semantics/article</dc:type><dc:identifier>https://doi.org/10.22146/ijc.21258</dc:identifier><dc:identifier>10.22146/ijc.21258</dc:identifier><dc:source>Indonesian Journal of Chemistry; Vol 14 No 2 (2014); 192-198</dc:source><dc:source>1411-9420</dc:source><dc:source>2460-1578</dc:source><dc:language>en</dc:language><dc:rights>https://creativecommons.org/licenses/by-nc-nd/4.0/</dc:rights></oai_dc:dc>